A round robin test aiming at measuring the high-temperature thermoelectric properties was carried out by a group of European (mainly French) laboratories (labs). Polycrystalline skutterudite Co0.97Ni0.03Sb3 was characterized by Seebeck coefficient (8 labs), electrical resistivity (9 labs), thermal diffusivity (6 labs), mass volume density (6 labs), and specific heat (6 labs) measurements. These data were statistically processed to determine the uncertainty on all these measured quantities as a function of temperature and combined to obtain an overall uncertainty on the thermal conductivity (product of thermal diffusivity by density and by specific heat) and on the thermoelectric figure of merit ZT. An increase with temperature of all these uncertainties is observed, in agreement with growing difficulties to measure these quantities when temperature increases. The uncertainties on the electrical resistivity and thermal diffusivity are most likely dominated by the uncertainty on the sample dimensions. The temperature-averaged (300–700 K) relative standard uncertainties at the confidence level of 68% amount to 6%, 8%, 11%, and 19% for the Seebeck coefficient, electrical resistivity, thermal conductivity, and figure of merit ZT, respectively. Thermal conductivity measurements appear as the least accurate. The moderate value of the temperature-averaged relative expanded (confidence level of 95%) uncertainty of 17% on the mean of ZT is essential in establishing Co0.97Ni0.03Sb3 as a high temperature standard n-type thermoelectric material.
Single crystals of SnSe have been reported to have very high thermoelectric efficiencies with a maximum figure merit zT = 2.5. This outstanding performance is due to ultralow thermal conductivities. We report on the synthesis of highly textured polycrystalline SnSe ingots with large single-crystal magnitude power factors, S2/ρ = 0.2–0.4 mW m−1 K−2 between 300–600 K, increasing to 0.9 mW m−1 K−2 at 800 K, and bulk thermal conductivity values κ300K = 1.5 W m−1 K−1. However, small SnSe ingots, which were measured in their entirety, were found to have a substantially reduced κ300K = 0.6 W m−1 K−1. Microscopy and diffraction revealed two distinct types of texturing within the hot-pressed ingots. In the interior, large coherent domains of SnSe platelets with a ∼45° orientation with respect to the pressing direction are found, while the platelets are preferentially oriented at 90° to the pressing direction at the top and bottom of the ingots. Fitting the κ(T) data suggests an increase in defect scattering for the smaller ingots, which is in keeping with the presence of regions of structural disorder due to the change in texturing. Combining the measured S2/ρ with the bulk ingot κ values yields zT = 1.1 at 873 K.
The complex impedance of a crystal has been measured. The frequency dependence is studied for a wide range of temperatures (50–403 K) and is found to be characteristic of relaxation process with a single Debye time relaxation constant, which is interpreted as a dielectric constant of the material. A strong peak is observed in this dielectric constant (up to at the charge ordering transition suggesting an interpretation in terms of ordering electric dipoles at or in term of phase separation. Comparison with —in which the phase separation is much smaller and the peak in the dielectric constant is absent—suggests an interpretation in term of phase separation between insulating and metallic states.