5 June 2007 in Journal of Electronic Materials
1 December 2017 in AIP Advances
Ti Schottky contacts were deposited on n-type 4H-SiC at different temperatures ranging from 28 oC to 900 oC using a magnetron sputtering deposition system to fabricate Schottky barrier diodes. Post deposition annealing at 500 oC for up to 60 hours in vacuum was carried to further improve the contact properties. Optimum barrier height of 1.13 eV and ideality factor of 1.04 was obtained in contacts deposited at 200 oC and annealed for 60 hours. Under a reverse voltage bias of 400 V, the average leakage current on these set of diodes was 6.6 x 10-8 A. Based on the x-ray diffraction analysis, TiC, Ti5Si3 and Ti3SiC2 were formed at the Ti/SiC interface. These results could be beneficial to improving the performance of 4H-SiC Schottky diodes for high power and high temperature applications.
12 March 2009 in Journal of Electronic Materials
11 March 2014 in Journal of Electronic Materials
1 February 2022 in AIP Advances
We report on the results of our investigation of the effect of deposition temperature on molybdenum (Mo) used as Schottky contacts to fabricate silicon carbide (SiC) Schottky barrier diodes. The contacts were deposited using magnetron sputtering on n-type 4H-SiC at temperatures ranging from 25 to 900 °C. The fabricated diodes were characterized by current–voltage, current–voltage–temperature, and capacitance–voltage measurements. The diodes showed average Schottky barrier heights that decreased from 1.54 to 1.00 eV with increasing deposition temperature of the contacts. The average values of the ideality factors similarly decreased from 1.21 to 1.06 with increasing deposition temperature. However, the diodes with contacts deposited at 400–900 °C nearly maintained a constant ideality factor value of 1.06. The x-ray diffraction analysis indicated that silicides were formed at the interface for contacts deposited at or above 400 °C. The improved properties of the diodes with contacts deposited at higher temperatures are correlated with the formation of the interfacial alloys possessing improved electrical properties. This work demonstrates that high temperature deposition is another method for optimizing the properties of Mo contacts for the fabrication of 4H-SiC Schottky diodes for electronic applications in high power and high temperature environments.