3 April 2021 in Journal of Asian Ceramic Societies
The thermal stability of MoAlB powder was studied. The effects of vacuum, Ar protection, molten salt treatment, and additives (B and C) on its thermal stability were studied. Results showed that MoAlB powder would react with a small amount of O2 in the furnace under vacuum and low temperature to form MoB, Al3Mo, B2O3, and Al2O3. At higher temperature, MoAlB first decomposed into MoB and Al. Al was oxidized to Al2O3. The thermal stability of MoAlB powder was better under the protection of Ar. However, molten salt heat treatment and additives such as B and C could promote the decomposition of MoAlB
20 December 2018 in Materials Research Express
Nanodiamonds with core/shell structures exhibit excellent adsorption and photocatalytic properties by annealing in an Ar atmosphere. Results show that the core/shell-structured nanodiamond/onion-like carbon materials were obtained at high-temperature annealing (1400 °C–1500 °C), and they possessed a good visible light photocatalytic activity. Solutions with 10 and 100 mg/L methyl orange could be almost completely degraded within 30 min and 1 h by the nanodiamonds annealed at 1500 °C, respectively.
1 August 2022 in Russian Journal of Non-Ferrous Metals
Mn/Al/B mixed powders were used as raw material for the thermal explosion reaction in a tubular furnace to rapidly prepare Mn2AlB2 ceramics with high conte
1 May 2018 in Journal of Superhard Materials
The Cu(Sn)–TiC x bonded diamond composites were prepared by in situ reaction sintering of Cu, Ti2SnC and diamond powders. Effect of Ti2SnC content on the phase composition, microstructure and...
2 January 2022 in Journal of Asian Ceramic Societies
Fe2AlB2 material was prepared through spark plasma sintering (SPS) by using Fe/Al/B mixed powder as the raw material. The effects of sintering temperature, holding time, and Al content on the phase composition and microstructure of the product were studied to obtain materials with high Fe2AlB2 content. Results showed that when the sintering temperature was increased to approximately 1000°C, SPS induced a thermal explosion reaction, resulting in the formation of a dense sintered sample with high Fe2AlB2 content. The sample contained a small amount of FeB and FeAl3 impurities. The synthesis of Fe2AlB2 could be promoted by optimizing holding time and increasing Al content in the raw materials. The most suitable process parameters for the synthesis of materials with high Fe2AlB2 content were 1000°C, no holding, and 2Fe/1.1Al/2B raw material. The Fe2AlB2 sample had good mechanical properties. Its Vickers hardness and bending strength were 10.5 GPa and 352 MPa, respectively. Given that the synthesized Fe2AlB2 material was unstable, continuously increasing the temperature or extending the holding time would cause it to decompose.
1 September 2019 in Materials Research Express
Sn21Cl16(OH)14O6 was prepared from SnCl2, NaOH, and surfactant powders through a simple solid-phase reaction method. The effects of surfactant addition on the phase compositions, morphologies, and photocatalytic properties of the photocatalyst were investigated. Results showed that the as-synthesized nanostructured Sn21Cl16(OH)14O6 had an average particle size of approximately 50–200 nm and a band gap of 3.82 eV. The addition of surfactants may promote the decomposition of Sn21Cl16(OH)14O6 into SnO and Sn and improve the photocatalytic property of Sn21Cl16(OH)14O6. The cetyltrimethylammonium bromide-modified sample possessed the best photocatalytic properties and degraded 98.9% of methyl orange within 60 min under visible-light irradiation.