We investigated a switchable ferroelectric diode effect and its physical mechanism in Pt/BiFeO/SrRuO thin-film capacitors. Our results of electrical measurements support that, near the Pt/BiFeO interface of as-grown samples, a defective layer (possibly an oxygen-vacancy-rich layer) becomes formed and disturbs carrier injection. We therefore used an electrical training process to obtain ferroelectric control of the diode polarity where, by changing the polarization direction using an external bias, we could switch the transport characteristics between forward and reverse diodes. Our system is characterized with a rectangular polarization-hysteresis loop with which we confirmed that the diode-polarity switching occurred at the ferroelectric coercive voltage. Moreover, we observed a simultaneous switching of the diode polarity and the associated photovoltaic response dependent on the ferroelectric domain configurations. Our detailed study suggests that the polarization charge can affect the Schottky barrier at the ferroelectric/metal interfaces, resulting in a modulation of the interfacial carrier injection. The amount of polarization-modulated carrier injection can affect the transition voltage value at which a space-charge-limited bulk current–voltage (–) behavior is changed from Ohmic (i.e., ∝ ) to nonlinear (i.e., ∝ with ≥ 2). This combination of bulk conduction and polarization-modulated carrier injection explains the detailed physical mechanism underlying the switchable diode effect in ferroelectric capacitors.
We investigated the ferroelectric domain-wall propagation in epitaxial thin film over a wide temperature range (3–300 K). We measured the domain-wall velocity under various electric fields and found that the velocity data is strongly nonlinear with electric fields, especially at low temperature. We found that, as one of surface growth issues, our domain-wall velocity data from ferroelectric epitaxial film could be classified into the creep, depinning, and flow regimes due to competition between disorder and elasticity. The measured values of velocity and dynamical exponents indicate that the ferroelectric domain walls in the epitaxial films are fractal and pinned by a disorder-induced local field.
We investigated the pinning dominated domain-wall dynamics under an ac field by studying the frequency dependence of hysteresis loops of a uniaxial ferroelectric (FE) system. We measured the fully saturated polarization-electric field hysteresis loops of high-quality epitaxial 100-nm-thick capacitors at various (5–2000 Hz) and temperatures (10–300 K). We observed that the coercive field is proportional to with two scaling regions, which was also reported earlier in magnetic systems [T. A. Moore and J. A. C. Bland, J. Phys.: Condens. Matter 16, R1369 (2004), and references therein]. In addition, we observed that the two scaling regions of vs exist at all measured . We found that the existence of the two scaling regions should come from a dynamic crossover between the creep and flow regimes of the FE domain-wall motions. By extending the theory of Nattermann et al., which was originally proposed for impure magnet systems [T. Nattermann, V. Pokrovsky, and V. M. Vinokur, Phys. Rev. Lett. 87, 197005 (2001)], to the disordered FE systems, we obtained analytical expressions for the dynamic crossovers between the relaxation and creep, and between the creep and flow regimes. By comparing with the experimental data from our fully saturated hysteresis loop measurements, we could construct a dynamic phase diagram with as a parameter for hysteretic FE domain dynamics in the presence of an ac field.
We investigated domain nucleation process in epitaxial capacitors under a modified piezoresponse force microscope. We obtained domain evolution images during polarization switching process and observed that domain nucleation occurs at particular sites. This inhomogeneous nucleation process should play an important role in an early stage of switching and under a high electric field. We found that the number of nuclei is linearly proportional to log(switching time), suggesting a broad distribution of activation energies for nucleation. The nucleation sites for a positive bias differ from those for a negative bias, indicating that most nucleation sites are located at the ferroelectric/electrode interfaces.