13 September 2023 in Advanced Science
Hydrogels are used in wound dressings because of their tissue‐like softness and biocompatibility. However, the clinical translation of hydrogels remains challenging because of their long‐term stability, water swellability, and poor tissue adhesiveness. Here, tannic acid (TA) is introduced into a double network (DN) hydrogel consisting of poly(vinyl alcohol) (PVA) and poly(acrylic acid) (PAA) to realize a tough, self‐healable, nonswellable, conformally tissue‐adhesive, hemostatic, and antibacterial hydrogel. The TA within the DN hydrogel forms a dynamic network, enabling rapid self‐healing (within 5 min) and offering effective energy dissipation for toughness and viscoelasticity. Furthermore, the hydrophobic moieties of TA provide a water‐shielding effect, rendering the hydrogel nonswellable. A simple chemical modification to the hydrogel further strengthens its interfacial adhesion with tissues (shear strength of ≈31 kPa). Interestingly, the TA also can serve as an effective hemostatic (blood‐clotting index of 58.40 ± 1.5) and antibacterial component, which are required for a successful wound dressing. The antibacterial effects of the hydrogel are tested against Escherichia coli and Staphylococcus aureus. Finally, the hydrogel is prepared in patch form and applied to a mouse model to test in vivo biocompatibility and hemostatic performances.
17 February 2023 in Advanced Science
Developing bioelectronics that retains their long‐term functionalities in the human body during daily activities is a current critical issue. To accomplish this, robust tissue adaptability and biointerfacing of bioelectronics should be achieved. Hydrogels have emerged as promising materials for bioelectronics that can softly adapt to and interface with tissues. However, hydrogels lack toughness, requisite electrical properties, and fabrication methodologies. Additionally, the water‐swellable property of hydrogels weakens their mechanical properties. In this work, an intrinsically nonswellable multifunctional hydrogel exhibiting tissue‐like moduli ranging from 10 to 100 kPa, toughness (400–873 J m−3), stretchability (≈1000% strain), and rapid self‐healing ability (within 5 min), is developed. The incorporation of carboxyl‐ and hydroxyl‐functionalized carbon nanotubes (fCNTs) ensures high conductivity of the hydrogel (≈40 S m−1), which can be maintained and recovered even after stretching or rupture. After a simple chemical modification, the hydrogel shows tissue‐adhesive properties (≈50 kPa) against the target tissues. Moreover, the hydrogel can be 3D printed with a high resolution (≈100 µm) through heat treatment owing to its shear‐thinning capacity, endowing it with fabrication versatility. The hydrogel is successfully applied to underwater electromyography (EMG) detection and ex vivo bladder expansion monitoring, demonstrating its potential for practical bioelectronics.
4 February 2025 in Advanced Materials Technologies
1 June 2026 in Advanced Functional Materials
Active stiffness, the changing of material stiffness in response to an external stimulus, can be harnessed for mechanically adaptive implantable devices and dynamic cell culture substrates for mechanobiology investigations. Conducting polymer (CP)‐based materials are capable of changing stiffness in response to an applied electrical potential: redox‐driven changes in charge state lead to ion transport and subsequent swelling. This phenomenon has been investigated for polymeric actuators but rarely for active stiffness. In this study, the stiffness of poly(3,4‐ethylenedioxythiophene): poly(styrenesulfonate) (PEDOT: PSS) films as a function of applied potential is characterized. Electrochemical preconditioning is first defined, and the proportionality of ion transport to voltage is identified. The maximum stiffness change observed over the potential range was found to be ∼32.5%, and changes of ∼6.7%–10.4% were found with 0.2 V increments. PEDOT: PSS films deviate in both their charge state and stiffness over a period of many hours after unbiasing. After unbiasing, PEDOT: PSS loses the transported charge over time and the stiffness changes by ∼2.6%–15.2% over 24 h. Finally, as a first step to evaluate the feasibility for biomedical applications, the active stiffness modulation process is determined to be cytocompatible. These characterizations highlight both the potential of CPs for active stiffness and identify areas for future optimization.