1 July 2014 in Catalysis in Industry
Verified
Journal Article
Closed access
PDF file
TBT. V. Bobkova
T. V. Bobkova
VDV. P. Doronin
V. P. Doronin
OPO. V. Potapenko
O. V. Potapenko
TST. P. Sorokina
T. P. Sorokina
NON. M. Ostrovskii
N. M. Ostrovskii
The effect of the content and nature of nitrogen compounds on the distribution of target products in transforming model hydrocarbons under cracking conditions over equilibrium zeolite-containing catalyst was studied. Using cracking of n-undecane as an example, a nearly 50% drop in the conversion and in yields of propane-propene (PPF) and butane-butene fractions (BBF) was observed when the pyrrol content in the feed was raised to 3000 ppm of nitrogen. Increasing the nitrogen content in the feed led to a nonlinear reduction in the rate constants of n-undecane cracking. It was found that the dependence of the yields of PPF, BBF, and isobutane in BBF on the conversion remained constant upon the cracking of n-undecane with various of nitrogen compounds; poisoning was likely to proceeds only because the acidic sites of the catalyst were blocked. The high poisoning effect of pyrrol and indole upon the cracking of n-undecane and decalin (strong proton donors) was observed along with the formation of ammonia. Quinoline exhibited high poisoning ability in the catalytic cracking of cumene with low [H]-donor activity. Quinoline poisoned catalysts to a greater degree than indole, during the catalytic cracking of non-hydrofined vacuum gasoil with a high content of aromatic structures. Indole exhibited the highest poisoning ability in processing heavy hydrocracking residue which was rich of paraffin-naphthene hydrocarbons.

4 August 2024 in Neftehimiâ
Verified
Journal Article
Closed access
PDF file
ОПОлег Валерьевич Потапенко
Олег Валерьевич Потапенко
ТБТатьяна Викторовна Бобкова
Татьяна Викторовна Бобкова
КДКонстантин Игоревич Дмитриев
Константин Игоревич Дмитриев
EKElena O. Kobzar
Elena O. Kobzar
ВДВладимир Павлович Доронин
Владимир Павлович Доронин
ВКВладислав Анатольевич Ковеза
Владислав Анатольевич Ковеза
Добавки к катализатору крекинга для снижения содержания токсичных компонентов в дымовых газах (обзор) Добавки к катализатору крекинга для снижения содержания токсичных компонентов в дымовых газах (обзор)

23 August 2018 in AIP Conference Proceedings
Verified
Conference Paper
Closed access
PDF file
TBT. V. Bobkova
T. V. Bobkova
OPO. V. Potapenko
O. V. Potapenko
VDV. P. Doronin
V. P. Doronin
TST. P. Sorokina
T. P. Sorokina
TGT. I. Gulyaeva
T. I. Gulyaeva
The effect of the rare earth elements (REEs) content in range from 0 to 3 wt.% in the cracking catalyst on n-undecane and cumene transformations in the presence of heterocyclic sulfur and nitrogen compounds was studied. The catalyst samples acidity increased at raising the REEs content in the catalysts up to 2 wt.%. The catalyst acidity was sharply reduced with a further increase in the REEs. This phenomenon led to an enhanced conversion of the feed and a decreased formation of highly poisonous nitrogen compounds. The relative conversions of n-undecane and cumene in the presence of nitrogen and sulfur compounds were 95 and 97 rel.%, accordingly.

18 March 2025 in Petroleum Chemistry
Verified
Journal Article
Closed access
PDF file
EKElena O. Kobzar
Elena O. Kobzar
VKV. A. Koveza
V. A. Koveza
TBT. V. Bobkova
T. V. Bobkova
OPO. V. Potapenko
O. V. Potapenko
A series of additives based on Fe(III)-modified MFI, FAU, and FER zeolites were investigated with focus on their efficiency in reducing NOx in cracking catalyst regeneration flue gases. The zeolite efficiency was found to depend on the zeolite framework type and the modification method. The Fe/MFI additives exhibited excellent performance. The additives prepared by ion exchange—and distinguished by uniform distribution of highly active metal ions (Fe3+)—reached a NOx reduction efficiency of 45.4%.

1 August 2022 in Petroleum Chemistry
Verified
Journal Article
Closed access
PDF file
AYA. S. Yurtaeva
A. S. Yurtaeva
OPO. V. Potapenko
O. V. Potapenko
TBT. V. Bobkova
T. V. Bobkova
TGT. I. Gulyaeva
T. I. Gulyaeva
The influence of the zinc incorporation method (ion exchange, impregnation) and its content (from 0.25 to 0.75 wt %) in ZSM-5 zeolite on the physicochemical characteristics of the zeolite (textural parameters, concentration of acid sites) and on the catalytic activity of cracking catalysts with the additives containing the modified zeolites in transformations of hydrotreated vacuum gasoil was studied. The zinc introduction by impregnation leads to a slight decrease in the zeolite specific surface area and micropore volume from 420 to 380 m2/g and from 0.131 to 0.117 cm3/g, respectively, and the total concentration of acid sites at the maximal zinc content increases by 17% compared to unmodified ZSM-5. Modification of the zeolite samples with zinc by ion exchange does not alter the main pore structure parameters compared to the initial zeolite, whereas the acid site concentration reaches the highest values (up to 2025 μmol/g). With an increase in the zinc content of ZSM-5 zeolite, with both modification methods (ion exchange, impregnation), the yield of the gasoline fraction and aromatic hydrocarbons in liquid products of cracking of hydrotreated vacuum gasoil increases.

1 October 2025 in Petroleum Chemistry
Verified
Journal Article
Closed access
PDF file
EKElena O. Kobzar
Elena O. Kobzar
VKV. A. Koveza
V. A. Koveza
TBT. V. Bobkova
T. V. Bobkova
TLTatyana Larina
Tatyana Larina
AAA. B. Arbuzov
A. B. Arbuzov
OPO. V. Potapenko
O. V. Potapenko
A series of additives based on an iron-modified MFI zeolite were investigated for their ability to reduce NOx in cracking catalyst regeneration flue gases. Their efficiency was dependent on the iron loading, the zeolite SiO2/Al2O3 ratio, and the initial cationic form used for modification. The Fe/MFI additives prepared from an NH4-form zeolite with a low SiO2/Al2O3 ratio (23) demonstrated excellent performance. Under industrially relevant catalyst regeneration conditions, the additive with an optimized iron oxide content (within a tested range of 0.5 to 2.5 wt %) reached a NOx reduction efficiency of 45.4%.