This study researched the effects of machining parameters on surface roughness and material removal rate in the wire electrical discharge cutting of high-density Al/B4C metal matrix composites produced via the hot pressing method. Wire tension, reinforcement percentage, wire speed, pulse-on time and pulse-off time were set as the control factors. The Taguchi L18 (21 × 34) orthogonal array was used in the experiment design and determination of the optimum control factors. Variance analysis was applied to determine the effects of the control factors on the surface roughness and material removal rate. The results showed the most effective parameters to be pulse-on time (30.22%) for surface roughness and wire speed (83.20%) for material removal rate, and the optimum levels of the control factors to be A2B1C2D1E1 and A2B2C3D2E2, respectively. Predictive equations were then developed by applying linear regression analysis, and the adjusted correlation coefficients were calculated as 0.61 for surface roughness and 0.785 for material removal rate.
8 June 2022 in Journal of the Brazilian Society of Mechanical Sciences and Engineering
Carbon fiber-reinforced Aluminum Laminate (CARALL) is a new generation of Fibre Metal Laminate (FML) material. This study investigates the low-velocity impact behavior of CARALL structures at different environmental temperatures (−40°C, 23°C, and 80°C). Two different groups of CARALL composite structures with varying fiber orientations were produced by hot pressing in a 3/2 arrangement: C1 (Al/0°90°/Al/90°0°/Al) and C2 (Al/0°0°/Al/0°0°/Al). Low-velocity impact tests were conducted at 23 J, 33 J, and 48 J energy levels using a Ø20 mm spherical impactor tip. The area of damage was detected by ultrasonic C-Scan. In addition, analysis of variance (ANOVA) was applied to reveal the influential parameters and their effect levels. After conducting experiments using the Taguchi L 18 test set, it was observed that the C2-coded specimen yielded better results in terms of maximum peak load, maximum displacement, and damage area. While the decrease in temperature increased the damage and maximum peak load, the increase in temperature did not cause a significant change in the maximum peak load. The primary damage mechanisms observed in damage investigations were matrix cracks and delamination between composite layers. Although delamination is present between the Al/CFRP layer, it is not significant. According to ANOVA results, impact energy was the most effective parameter for maximum impact force, maximum displacement, and damage area, with contribution rates of 81%, 74%, and 76%, respectively. The optimal experimental conditions (23°C temperature and 23 J impact energy with the C1-coded sample) were determined using grey relational analysis based on principal component analysis.
In this study, the effects of particle addition on the microstructure, mechanical properties and fracture behaviors of Al/B4C particle reinforced composite produced by hot pressing method were investigated. After the production of 5, 10 and 15 wt.-% of B4C reinforced composites, T6 heat treatment was applied. It was specified that a strong interface bond occurred between the matrix and particles, and during the fracturing of composites, this effect increased the particle fracture. It was observed that particles were fractured parallel to the fracture surface and to each other fracture surface of MMCp. In general, cavity of particle separated from the matrix was not seen. In the production of MMCp, it was also observed that hot pressing provided a density higher than 99 %. After the heat treatment the maximum hardness value of 173 HB was reached with 15 wt.-% B4C reinforced sample. The transverse rupture strength (TRS) decreased with the increase of reinforcement ratio. The highest TRS was 510 MPa with the 5 wt.-% reinforced material, whereas the lowest value was obtained to be 387 MPa with the 15 wt.-% B4C reinforced material.