Mihkel Vestli

Mihkel Vestli

Auto-generated profile, based on publicly available information

Mihkel Vestli

Institute of Chemistry, University of Tartu, 50411 Tartu, Estonia

Research Focus & Metrics

Academic Career Length

16Years (2011-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 January 2012 in Journal of the Electrochemical Society
Verified
Journal Article
Closed access
PDF file
HKH. Kurig
H. Kurig
MVM. Vestli
M. Vestli
KTK. Tõnurist
K. Tõnurist
AJAlar Jänes
Alar Jänes
ELE. Lust
E. Lust
Various ionic liquids based on 1-ethyl-3-methylimidazolium cation and tetrafluoroborate, tetracyanoborate, tris(pentafluoroethyl)trisfluorophosphate, bis(trifluoromethylsulfonyl)imide, bis(fluorosulfonyl)imide, and thiocyanate anions have been studied as electrolytes in two electrode supercapacitor test cells based on carbon cloth electrodes. Three electrode test cells were also completed and studied to analyze the processes taking place on electrode|electrolyte interface at different electrode potentials. Electrical double layer formation and adsorption kinetics of ions onto electrode surface and mass-transfer processes in porous electrode and separator matrix, dependent on the conductivity, viscosity and melting temperature of ionic liquids, have been analyzed using impedance and cyclic voltammetry data. Electrical charge delocalization has been calculated and discussed to point out and explain differences in the behavior of ionic liquids as supercapacitor electrolyte at different electrode potentials. Suitability of 1-ethyl-3-methylimidazolium tetrafluoroborate and 1-ethyl-3-methylimidazolium tetracyanoborate ionic liquids as electrolytes for supercapacitors has been demonstrated.

1 January 2011 in Electrochemical and Solid-State Letters
Verified
Journal Article
Closed access
PDF file
HKH. Kurig
H. Kurig
MVM. Vestli
M. Vestli
AJA. JänEs
A. JänEs
ELEnn Lust
Enn Lust
The electrochemical characteristics for the electrical double layer capacitors (EDLCs) based on the microporous carbon cloth (MPCC) electrode and 1-ethyl-3-methyl imidazolium tetrafluoroborate or 1-ethyl-3-methyl imidazolium tetracyanoborate as an electrolyte have been studied using the cyclic voltammetry and impedance spectroscopy methods. The considerable dependence of gravimetric series capacitance, phase angle, power and energy densities on the composition of the anion in room-temperature ionic liquid (RTIL) have been demonstrated. The region of ideal polarisability for both MPCC|RTIL EDLCs is up to 3.2 V.

18 November 2015 in Journal of the Electrochemical Society
Verified
Journal Article
Open access
PDF file
GNGunnar Nurk
Gunnar Nurk
MVM. Vestli
M. Vestli
PMP. Möller
P. Möller
RJRaivo Jaaniso
Raivo Jaaniso
MKM. Kodu
M. Kodu
ELE. Lust
E. Lust
Gadolinia doped ceria Ce0.9Gd0.1O2-δ (GDC) barrier layer was deposited onto YSZ electrolyte and Ni-YSZ|YSZ electrolyte half-cell using pulsed laser deposition (PLD), magnetron sputtering (MS) or spray pyrolysis (SP) methods. The first set of GDC barrier layers was studied without additional sintering and the second set was additionally sintered for 3 h at 1300°C. Sr mobility initiated by thermal treatment of La0.6Sr0.4CoO3-δ cathode at 950°C and 1100°C was systematically studied with the GDC layers prepared using PLD, MS and SP methods. Concentration profiles of Zr ion in GDC, Ce in YSZ, Sr in GDC and Sr in YSZ were recorded using TOF-SIMS analysis method. XRD and SEM methods were applied for the analysis of Sr mobility in the GDC layer and results were correlated with impedance, cyclic voltammetry and other electrochemical data. The influence of synthesis method and thermal treatment of the GDC layer on the Sr mobility was established. Changes in the microstructure of cathode|chemical barrier layer|electrolyte interfaces caused by the thermal treatment of the cathode as well as the GDC layer during the preparation (including sintering) steps have been demonstrated and discussed.

5 May 2015 in Journal of the Electrochemical Society
Verified
Journal Article
Closed access
PDF file
MVMihkel Vestli
Mihkel Vestli
ELEnn Lust
Enn Lust
GNGunnar Nurk
Gunnar Nurk
Tb and Sm cation binary co-doped ceria films were deposited using the ultrasonic atomizing spray pyrolysis method. Crack-free homogenous films with different dopant concentrations were deposited and thereafter annealed at fixed temperatures T = 900, 1200 and 1300°C, respectively. It was demonstrated that several microstructural parameters of oxide films are controlled by the sintering temperature. The Ce0.9Sm0.1-xTbxO2-δ films formed were analyzed using X-ray diffraction, scanning electron microscopy, high resolution transmission electron microscopy, atomic force microscopy and a four probe DC technique at different pO2 and temperature conditions. Based on the SEM analysis the average thickness of the Ce0.9Sm0.1-xTbxO2-δ films was approximately 700 nm. The XRD patterns for the Ce0.9Sm0.1-xTbxO2-δ films annealed at 1200°C indicated a high degree of crystallinity. Tb dopant ions influence the microstructural properties like median diameter of grains, microstrain, lattice parameter and electrical properties like activation energies of ionic and electronic part of conductivity for the Ce0.9Sm0.1-xTbxO2-δ film. A significantly higher microstrain value for the lowest Tb dopant concentration with accompanied change in electrical properties was observed.

2 June 2015 in ECS Transactions
Verified
Journal Article
Closed access
PDF file
GNGunnar Nurk
Gunnar Nurk
PMPriit Möller
Priit Möller
MVMihkel Vestli
Mihkel Vestli
RJRaivo Jaaniso
Raivo Jaaniso
MKMargus Kodu
Margus Kodu
ELEnn Lust
Enn Lust
Gadolinia doped ceria Ce0.9Gd0.1O2- d (GDC) barrier layers with thickness approximately 0.7 mm were deposited onto the YSZ electrolyte using pulsed laser deposition (PLD), magnetron sputtering (MS) and spray pyrolysis (SP) method. One set of layers were studied without additional sintering and other set were sintered for 30 h at 1300 °C before using as barrier layer. Sr mobility from Pr0.6Sr0.4CoO3- d and La0.6Sr0.4CoO3- d cathodes through PLD, MS and SP layers caused by thermal treatment at 950 °C and at 1100 °C, respectively, were systematically studied. Concentration profiles of Zr ion in GDC, Ce in YSZ, Sr in GDC and Sr in YSZ were recorded using TOF-SIMS analysis. XRD, SEM and electrochemical studies were performed. Influence of synthesis method and thermal treatment of layer on the Sr mobility was demonstrated. Changes in layer microstructure caused by thermal treatment of cathode as well as GDC layer during preparation were demonstrated.

1 January 2011 in Electrochemical and Solid-State Letters
Verified
Journal Article
Closed access
PDF file
HKH. Kurig
H. Kurig
MVM. Vestli
M. Vestli
AJA. Jänes
A. Jänes
ELE. Lust
E. Lust