Yizheng Feng

Yizheng Feng

Auto-generated profile, based on publicly available information

Yizheng Feng

Jiangsu Univ Sci & Technol, Coll Mat Sci & Engn, Zhenjiang 212100, Peoples R China

Research Focus & Metrics

Academic Career Length

3Years (2024-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
20 June 2024 in Physica Scripta
Verified
Journal Article
Closed access
YFYizheng Feng
Yizheng Feng
XXXiangping Xu
Xiangping Xu
XWXiling Wang
Xiling Wang
LWLingyu Wang
Lingyu Wang
JZJiasheng Zou
Jiasheng Zou
ZWZiqing Wang
Ziqing Wang
This study utilised self-developed ER90S-G wires for butt welding tests on AG728 plates to investigate the influence of heat treatment on the microstructure and mechanical properties of welded joints. Furthermore, it aimed to analyse the microstructure and metallurgical mechanisms of these joints. The findings reveal that the microstructure of the welded joints primarily consists of acicular ferrite with a minor presence of granular bainite. Following heat treatment, there is a noticeable growth in acicular ferrite and the emergence of tempered sorbite and massive ferrite; concurrently, austenite grain boundaries vanish, carbide aggregation increases, the quantity of large angular grain boundaries diminishes, and the martensite–austenite constituent elements gradually disappear. The physical phase of the base material, the heat-affected zone (HAZ), and the welded joints uniformly transition to α-Fe. Additionally, inclusions measuring 0.5 μm, predominantly MnSiO3, evidently promote the formation of ferrite. The tensile strength and impact toughness experience a minor reduction while the hardness of the HAZ and weld seam significantly decreases. The micro-morphology of the welded joint’s tensile fracture is predominantly characterised by dimples, within which inclusions or precipitated phase particles are distinctly visible, indicating a microporous coalescence-type fracture. At −45 °C, the impact test of welded joints reveals that the HAZ impact fracture micro-morphology exhibits brittle deconstructive fracture patterns, which, through heat treatment, transition to quasi-cleavage characteristics with reduced and shorter river patterns. The base material and weld fracture micro-morphology are primarily defined by the presence of dimples.

5 December 2024 in Physica Scripta
Verified
Journal Article
Closed access
SMShangbo Ma
Shangbo Ma
XXXiangping Xu
Xiangping Xu
XWXiling Wang
Xiling Wang
YFYizheng Feng
Yizheng Feng
CXChunzhi Xia
Chunzhi Xia
HTHong Teng
Hong Teng
A nickel-based WC-10Ni composite coating was fabricated via vacuum brazing at 1160 °C, using TC4 titanium alloy as the matrix, WC-10Ni powder as the hard phase, and BNi-5 as the brazing material. The study examined the coating’s microstructure and analyzed the impact of the WC-10Ni ratio and friction test temperature on its wear resistance, alongside a discussion of the wear mechanism. The results revealed that the hard layer of the composite coating comprised TiC, W, and minor amounts of Ti5Si3 and α-Ti, while the interface layer displayed a network structure of Ti2Ni and Ti5Si3. Using a Si3N4 ceramic ball as the counter-wear material, under conditions of a 10N load, 318 r min−1 rotational speed, 3 mm wear radius, and 30 min wear duration, the average friction coefficients of the three composite coatings were 0.289, 0.241, and 0.271, and their wear rates were 65.8%, 39.7%, and 52.7% of the substrate, respectively. The 50% WC-10Ni coating exhibited the best wear resistance, with adhesive wear being the dominant mechanism, accompanied by minor abrasive wear. Friction tests on the 50% WC-10Ni coating at 200 °C, 400 °C, 600 °C, and 800 °C revealed that the lowest wear rate, 0.35 × 10−5 mm3 N−1 m−1, occurred at 600 °C, where the average friction coefficient was 0.432 and oxidative wear was predominant. At 800 °C, the coating suffered significant damage, resulting in deteriorated wear resistance.