In this article we present a detailed study of the electronic structure from various Mn-based Heusler alloys using x-ray photoelectron spectroscopy (XPS) and x-ray emission spectroscopy (XES) techniques. Performing the measurements on the Mn- core levels as well as on the valence-band states we arrive at a more or less complete description of the electronic and magnetic properties of these compounds. The experimental Mn- spectra have been compared with fully relativistic photoemission calculations, which are based on the solution of the spin-polarized Dirac equation. The almost constant exchange splitting of about 0.35 eV, measured between the different Mn- sublevels is explainable in terms of the local magnetic moment at the Mn site. Moreover a strong relationship between the magnetization direction and the line shapes of the calculated Mn- core-level spectra has been revealed from our analysis. Depending on the atomic number of the Z element we obtain from XES experiments an increasing localization of the Mn- states. Also the interatomic distances in the different alloys seem to play an important rule in this process. To support this result we performed in addition valence-band measurements by applying XP. These data, which agree very well with the corresponding x-ray emission spectra are quantitatively reproduced from first-principle electronic structure calculations.
The temperature dependences of the resistivity, Hall coefficient, and magnetic susceptibility of iron-vanadium-aluminum alloys have been investigated. It has been established that the alloy exhibits semiconductor behavior for the method used to obtain uniform alloys. It is shown that at temperatures below the semiconductor alloy possesses the characteristic low-temperature scale of the dependences observed, which could be responsible for the appearance of a narrow pseudogap in the electron density of states. A simple theoretical description of the effects of a pseudogap is proposed. A consistent fit of the theoretical to the experimental relations made it possible to determine the effective width of the pseudogap and its relative depth .