5 October 2007 in Physical Review Letters
We develop a nucleation-based model to explain the formation of the wurtzite phase during the catalyzed growth of freestanding nanowires of zinc blende semiconductors. We show that in vapor-liquid-solid nanowire growth, nucleation generally occurs preferentially at the triple phase line. This entails major differences between zinc blende and wurtzite nuclei. Depending on the pertinent interface energies, wurtzite nucleation is favored at high liquid supersaturation. This explains our systematic observation of zinc blende during early growth of gold-catalyzed GaAs nanowires.
1 December 2008 in Physical Review B
Theoretical model for the growth of semiconductor nanowires is developed, which enables one to determine the growth conditions under which the formation of nanowires is possible. General expression for the nanowire growth rate as function of its radius and the growth conditions is obtained and analyzed. The model also describes the transformation from cubic to hexagonal crystal phase of nanowires. It is shown that the observed crystal structure is controlled mainly by the growth kinetics. Structural diagrams and probabilities of cubic and hexagonal phase formation are calculated as functions of supersaturation and nanowire radius within the plausible range of material parameters. Numerical estimates for the domains of phase mixing and phase purity are presented and analyzed.
5 March 2010 in Nano Letters
7 November 2005 in Applied Physics Letters
GaAs nanowires were grown by molecular-beam epitaxy on (111)B oriented surfaces, after the deposition of Au nanoparticles. Different growth durations and different growth terminations were tested. After the growth of the nanowires, the structure and the composition of the metallic particles were analyzed by transmission electron microscopy and energy dispersive x-ray spectroscopy. We identified three different metallic compounds: the hexagonal structure, the orthorhombic AuGa structure, and an almost pure Au face centered cubic structure. We explain how these different solid phases are related to the growth history of the samples. It is concluded that during the wire growth, the metallic particles are liquid, in agreement with the generally accepted vapor-liquid-solid mechanism. In addition, the analysis of the wire morphology indicates that Ga adatoms migrate along the wire sidewalls with a mean length of about .
8 November 2013 in Physical Review B
We develop a quantitative model of the self-catalyzed vapor-liquid-solid growth of GaAs nanowires, that depends on only a few a priori unknown physical parameters. The model is based on the sole consideration of the As species and incorporates all relevant mechanisms of exchange of As between the vapor, liquid, and solid phases, namely direct impingement of molecules on the droplet, their re-emission by the neighboring surfaces, evaporation from the droplet, and nucleation at the solid-liquid interface. It reproduces quantitatively all salient features of our experimental study, namely the variations of nanowire growth rate with As flux, temperature, and nanowire radius. From these optimized fits, we extract a complete set of model parameters, in particular the nucleus edge energy. We also determine quantities so far inaccessible to experiment, such as the As concentration in the droplet (about 1%), supersaturation of the liquid, and nucleation barrier, for individual nanowires. The model can then be used to predict the growth rate (and all quantities of interest) for an arbitrary GaAs nanowire of given geometry in arbitrary growth conditions, including conditions not yet explored experimentally, provided the fraction of the As flux re-emitted by its environment is known. Although largely ignoring group III elements, our model captures most of the physics of self-catalyzed nanowire growth.
14 February 2006 in Physical Review E
A theoretical model of nanowire formation by the vapor-liquid-solid mechanism during molecular beam epitaxy and related growth techniques is presented. The model unifies the conventional adsorption-induced model, the diffusion-induced model, and the model of nucleation-mediated growth on the liquid-solid interface. The concentration of deposit atoms in the liquid alloy, the nanowire diameter, and all other characteristics of the growth process are treated dynamically as functions of the growth time. The model provides theoretical length-diameter dependences of nanowires and the dependence of the nanowire length on the technologically controlled growth conditions, such as the surface temperature and the deposition thickness. In particular, it is shown that the length-diameter curves of nanowires might convert from decreasing to increasing at a certain critical diameter and that the nanowires taper when their length becomes comparable with the adatom diffusion length on the sidewalls. The theoretical dependence of the nanowire morphology on its lateral size and length and on the surface temperature are compared to the available experimental data obtained recently for Si and nanowires.