Increasingly extreme environmental conditions demand structural materials that combine mechanical robustness with sustainability. Natural wood is renewable and mechanically adaptable but suffers from high porosity and hydrophilicity, leading to moisture absorption, fire vulnerability, and environmental degradation. Ceramics provide high stiffness, thermal stability, and chemical resistance but are inherently brittle. Here we report ceramic wood, a composite formed by integrating a natural wood scaffold with uniformly distributed ceramic nanoparticles. A calcium silicate precursor infiltrates the aligned nanofluidic channels of wood and undergoes in-situ self-assembly into calcium silicate hydrate nanoparticles under room-temperature conditions. The resulting ceramic network fills micropores and forms strong interfacial bonding within the wood scaffold. Ceramic wood exhibits high compressive strength, enhanced toughness, excellent fire resistance, and improved durability against moisture, fungi attack, and alkaline environments. CO₂ uptake further reduces the carbon footprint, highlighting ceramic wood as a sustainable structural material for extreme environments.
Basic oxygen furnace (BOF) steel slag has potential as a supplementary cementitious material (SCM), but its low reactivity limits its application. In this study, BOF slag was treated with a high dosage of oxalic acid to produce a modified slag, denoted as Ox-BOF, which exhibited a refined particle size distribution and stored a significant amount of carbon. The performance of Ox-BOF as an SCM was evaluated. When used as a partial cement replacement, Ox-BOF resulted in slightly reduced flowability, prolonged setting time, and improved compressive strength, particularly at high replacement ratios and a late age of 28 days, as compared with the untreated BOF slag. The results demonstrate that oxalic acid treatment provides a promising approach for enhancing the utilization of BOF slag as an SCM, enhancing industrial sustainability.