Spatial structure of high-density radio frequency ring-shaped magnetized discharge plasma sputtering with two facing ZnO/Al2O3 cylindrical targets mounted in ring-shaped hollow cathode has been measured and Al-doped ZnO (AZO) thin film is deposited without substrate heating. The plasma density has a peak at ring-shaped hollow trench near the cathode. The radial profile becomes uniform with increasing the distance from the target cathode. A low ion current flowing to the substrate of 0.19 mA/cm2 is attained. Large area AZO films with a resistivity of 4.1 – 6.7×10-4 Ω cm can be prepared at a substrate room temperature. The transmittance is 84.5 % in a visible region. The surface roughnesses of AZO films are 0.86, 0.68, 0.64, 1.7 nm at radial positions of r = 0, 15, 30, 40 mm, respectively, while diffraction peak of AZO films is 34.26°. The grains exhibit a preferential orientation along (002) axis.
1 June 2006 in Japanese Journal of Applied Physics
Magnetron sputtering generally increases the temperature of the substrate placed to face the sputtering target above 40 °C because the plasmas are transported through unbalanced magnetic field lines from the sputtering target to the substrate surface. However, by using a magnetic mirror-type magnetron cathode, we were able to suppress the temperature of the substrate temperature to the environmental temperature of less than 40 °C at a target–substrate distance of 50 mm with a DC input power of 30 W and an Ar gas pressure of 0.15 Pa. This was possible because the balanced magnetic field lines confined the plasmas near the sputtering target. By enabling film deposition on low heat-resistant substrates, this deposition technique for suppressing the substrate temperature may have uses in various application fields.
A novel magnetron sputtering cathode with a magnetic mirror configuration is proposed, for low power density operation. The magnetic field profiles are simply constructed using two cylindrical permanent magnets positioned behind the disk-shaped sputtering target of 50 mm in diameter. The magnetic mirror configuration near the center and the outer edges of the target enables low power density operation up to 0.25 W/cm2 in the case of DC input power of 5 W. A sputtering rate of ∼0.2 nm/min was obtained under experimental conditions with target-substrate distance of 280 mm, Ar gas pressure of 0.1 Pa, and DC input power of 15 W.