This paper describes the structural and textural characteristics of silicon oxycarbide ceramics obtained from three different hybrid polymers by varying pyrolysis temperature. The first polymer was prepared by hydrosilylation between poly(hydromethylsiloxane) and divinylbenzene in stoichiometric proportions; the second was similarly obtained, but with excess of divinylbenzene (60 wt.%) and the third was also synthesized with 60 wt.% divinylbenzene, involving simultaneously hydrosilylation and radical reactions. Precursors were pyrolysed under argon at 1000, 1200 and 1500°C to produce silicon oxycarbide-based ceramics. Silicon carbide phase development and devitrification resistance were influenced by the disordered and ordered residual carbon fraction, which was directly related to the polymer structure. High specific surface area and pore volume values were obtained in C-richer ceramics at 1500°C derived from poly(divinylbenzene) network-containing precursor. Silicon oxycarbide matrices, derived from hybrid polymers containing graphitic carbon and silicon carbide phases together with different amount of porosity, revealed desirable features for electrochemical applications and adsorbent systems.
5 September 2024 in Journal of Solid State Electrochemistry
Silicon oxycarbide (SiCO) ceramics obtained from polymer pyrolysis and with varied carbon contents were prepared and evaluated as new electrodic materials for sensing of tert‑butylhydroquinone (TBHQ) and butylated hydroxyanisole (BHA) antioxidants. Three polymers were synthesized varying molecular architecture and aromatic carbon groups, followed by pyrolysis at 1000 and 1500 °C to obtain SiCO ceramics. Graphitization and crystallization processes were evidenced, in different extent, according to precursor chemistry. SiCO at 1500 °C with intermediary carbon content provided slight improvement in the peak anodic separation of TBHQ and BHA and higher peak current compared with glassy carbon electrode (GCE). Higher acidic sites concentration together with more ordered residual carbon phase produced in situ contributed to great electrochemical performance of SiCO towards phenolic compounds detection. Therefore, the ceramic herein prepared exhibits highly efficient features as a new SiCO composited electrode for simultaneous determination of antioxidant phenolic compounds bearing in mind further analytical applications.
1 January 2021 in Journal of the Brazilian Chemical Society
This work deals on the preparation of silicon oxycarbide (SiOC) and silicon boron oxycarbide (SiBOC) ceramics from pyrolysis involving alkoxysilanes with different organic groups. Boron content, organic substituent and annealing time were evaluated on crystallization and composition of resulting ceramics. B-free precursors composed of methyltriethoxysilane (MTES), phenyltriethoxysilane (PTES) and vinyltrimethoxysilane (VTMS) were obtained by the sol-gel method, whilst B-containing precursors were prepared by adding to each alkoxysilane a proper amount of boric acid resulting in B/Si atomic ratios of 0.1 and 0.5. Precursors were pyrolyzed at 1500 °C for 1 and 3 h to produce respective SiOC and SiBOC ceramics. X-ray diffraction (XRD) patterns revealed enhanced SiC phase crystallization for PTES-derived ceramics, followed by those containing vinyl and methyl groups, which was also confirmed by X-ray photoelectron spectroscopy (XPS) from percentages of Si-C and Si-O bonds. Csp2 and Csp3 amounts varied among ceramics, indicating direct influence of organic substituent on conductive carbon phase development. Boron addition induced the growth of SiC crystallites, having more evident effect in matrices with higher proportions of amorphous fraction and lower residual carbon amounts. Organic group nature, boron content and annealing time played an important role for production and evolution of SiC and C phases into ceramics.