Yttrium scandate crystal fiber has been obtained through laser-heated pedestal growth. The crystal belongs to a bixbyite crystal structure and crystallizes in Ia space group. X-ray diffraction method shows a lattice parameter of a = 10.228(1) Å. Factor-group analysis of YScO3 Raman spectra points to high degree of disorder in crystal structure of the new compound. Spectral-kinetic investigation of the crystal fibers doped by rare-earth ions points to the presence of two independent active optical centers of rare-earth ions. Moreover, the character of rare-earth impurities’ distribution is independent on a rare-earth ionic radius size.
Yttrium scandate crystals doped by Nd3+ and Tm3+ ions have been successfully grown in the form of fibers using the laser-heated pedestal growth (LHPG) technique. The selective laser spectroscopy methods have identified and distinguished three distinct types of optically active centers associated with Nd3+ and Tm3+ ions. The substitution of Y3+ and Sc3+ for rare-earth ions in the C2 structural site leads to the formation of two distinct basic long-time centers. In Nd3+:YScO3, another type of center (a short-lifetime one) is formed known as the Nd3+–Nd3+ aggregate pair. This center arises from the substitution of Y3+ or Sc3+ for Nd3+ cation in the adjacent MO6 polyhedra that share an edge. In Tm3+:YScO3, the third optical center is formed as a result of the substitution of Y3+ or Sc3+ for Tm3+ in the MO6 octahedra with the C3i site symmetry. The fluorescence decay lifetimes of Nd3+ and Tm3+ ions in the YScO3 crystal structure have been accurately measured and estimated. A Stark level diagram illustrating the splitting of 4F3/2, 4I11/2, and 4I9/2 multiplets of Nd3+ ions has been constructed to show features of the active optical centers with the C2 site symmetry.
A setup is developed for measuring optical characteristics of opaque and translucent solids in the temperature range of 25 to 1600°C and spectral range of 0.65 to 10.6 µm. Procedures of calibration experiments and measurements of spectral and integral emissivity are described. These procedures allow spectral and integral emissivity and spectral and integral reflectances of various materials, including translucent ones, to be measured accurate to about 10% in the spectral range of 0.65 to 10,6 µm and temperature range of 25 to 1600°C. Optical characteristics of materials are measured at the atmospheric pressure in the normal oxygen atmosphere or in the atmosphere with reduced oxygen content (inert gas or carbon dioxide blowing on the frontal surface of the samples). The accuracy of the thus obtained data on temperature and spectrum dependences of optical characteristics of materials allow measurements to be performed for developing various structures capable of operating at high temperatures.
Yttrium scandate crystals doped by Nd3+ and Tm3+ ions have been obtained in the form of a fiber through the laser-heated pedestal growth (LHPG) method. Three types of optical centers of Nd3+ and Tm3+ have been recorded by the selective laser spectroscopy methods. Two dominant centers form due to substitution of the rare-earth ions for Y3+ and Sc3+ in the structural site of C2. In the case of Nd3+:YScO3, the third one is aggregate pair center Nd3+ - Nd3+ which forms due to substitution of basic ions (Y3+ or Sc3+) in neighboring MO6 polyhedra shared the edge. In the case of Tm3+:YScO3, the third optical center form due to substitution of Tm3+ for Y3+ or Sc3+ in the octahedra MO6 with symmetry site of C3i. The lifetime have been estimated for Nd3+ and Tm3+ ions occupied MO6 polyhedra with symmetry sites of C2 and C3i in the YScO3 crystal fibers. Stark level schematic of 2F3/2, 4I11/2, and 4I9/2 multiplets of Nd3+ ions have been built for both centers of C2 in the YScO3 crystal fiber