Single phase, adherent films of copper oxide nanowires (CuO NWs) were successfully grown on a glass substrate. Titanium nanofilm was pre-coated on the glass substrate to assist the growth of a layer adherent to the substrate. The copper film of 1.5 μm thickness was deposited via physical vapor deposition technique followed by thermal oxidation in air at various temperatures for 4 h. The product was characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), ultraviolet-visible (UV-Vis) and Fourier transformation infrared (FT-IR) spectroscopy to find the crystal structure, morphology, phases, and optical properties of the deposited films. The CuO NWs film with 60% transmittance at wavelengths greater than 800 nm was obtained. It can be used as an infrared thermal imaging filter and in optoelectronic devices. The fabricated temperature sensor exhibited high sensitivity in the temperature range of 20 °C to 180 °C.
30 May 2020 in Journal of Inorganic and Organometallic Polymers and Materials
FDFaisal Abdulqader Dawood
27 November 2025 in Plasmonics
8 September 2020 in Baghdad Science Journal
Sn effect on the phase transformation behavior, microstructure, and micro hardness of equiatomic Ni-Ti shape memory alloy was studied. NiTi and NiTiSn alloys were produced using vacuum induction melting process with alloys composition (50% at. Ni, 50% at.Ti) and (Ni 48% at., Ti 50% at., Sn 2% at.). The characteristics of both alloys were investigated by utilizing Differential Scanning Calorimetry, X- ray Diffraction Analysis, Scanning Electron Microscope, optical microscope and vicker's micro hardness test. The results showed that adding Sn element leads to decrease the phase transformation temperatures evidently. Both alloy samples contain NiTi matrix phase and Ti2Ni secondary phase, but the Ti2Ni phase content decreases with Sn addition and this is one of the reasons that leads to decrease the micro hardness of alloy with adding Sn element in a noticeable manner. The micro hardness decreases from 238.74 for NiTi equiatomic alloy to 202 for NiTiSn alloy after heat treatment.