Safe, fast, and energy efficient cycling of lithium ion batteries is desired in many practical applications. However, modeling studies predict steep Li+ ion gradients in the electrodes during cycling at the higher currents. Such gradients introduce heterogeneities in the electrodes, which make it difficult to predict cell lifetimes as different portions of the cell age at different rates. There is a dearth of experimental methods to probe these concentration gradients across the depth of the electrode. Here we use spatially resolved energy dispersive X-ray diffraction to obtain a “movie” of lithiation and delithiation in different sections of the cell and quantify lithium gradients that develop in a porous graphite electrode during cycling at a 1C rate. Inhomogeneity in the total Li content, and in the individual ordered LixC6 phases formed during lithium insertion into (and extraction from) the graphite, has been observed in an operando fashion. The complex dynamics of lithium-staging in graphite with the distinct front propagation of phase changes have been characterized and new features of these dynamics are highlighted here. As large Li+ ion gradients contribute to cell polarization, our results suggest that Li plating conditions can be met near the graphite electrode surface, even when the cell is charged at a moderate (1C) rate.
27 March 2019 in Journal of the Electrochemical Society
Nickel-rich Ni-Co-Mn (NCM) or Ni-Co-Al (NCA) layered-oxide positive electrodes (cathodes) allow high-voltage operation of lithium-ion cells with increased energy density, but their long-term cycling causes gradual increase in their impedance that slows down lithiation and delithiation of the material. Here we report that pairing of these cathodes with lithium titanate (Li4Ti5O12, LTO) negative electrodes (anodes) accelerates this impedance rise when compared to pairing with graphite (Gr) electrodes, during potentiostatic holds (calendar-aging) at sufficiently high (> 4.2 V vs. Li/Li+) layered-oxide potentials. Our results suggest that gases generated in the cell play an important role in this impedance rise. In the graphite cells, these gases are gradually depleted by reactions at the Gr electrode, but such reactions do not occur at the LTO electrode. The generation and buildup of gases degrades the electron conduction network within the cathode, and also leads to modifications at the oxide-electrolyte interfaces, causing the observed impedance rise. The calendar-aging also alters cell capacity, with losses observed in the Gr cells and gains observed in the LTO cells. Possible causes and consequences of these changes in the lithium-ion inventory of the cells are discussed.
13 January 2014 in ACS Applied Materials & Interfaces