17 September 2021 in Science Advances
The carrier alternation from Li atoms to Li vacancies leads to interface instability in solid-state lithium alloy anodes.
23 November 2022 in Science Advances
In the pursuit of energy-dense all-solid-state lithium batteries (ASSBs), Li-rich Mn-based oxide (LRMO) cathodes provide an exciting path forward with unexpectedly high capacity, low cost, and excellent processibility. However, the cause for LRMO|solid electrolyte interfacial degradation remains a mystery, hindering the application of LRMO-based ASSBs. Here, we first reveal that the surface oxygen instability of LRMO is the driving force for interfacial degradation, which severely blocks the interfacial Li-ion transport and triggers fast battery failure. By replacing the charge compensation of surface oxygen with sulfite, the overoxidation and interfacial degradation can be effectively prevented, therefore achieving a high specific capacity (~248 mAh g −1 , 1.1 mAh cm −2 ; ~225 mAh g −1 , 2.9 mAh cm −2 ) and excellent long-term cycling stability of >300 cycles with 81.2% capacity retention at room temperature. These findings emphasize the importance of irreversible anion reactions in interfacial failure and provide fresh insights into constructing stable interfaces in LRMO-based ASSBs.
11 November 2022 in Science Advances
The fundamental understanding of the elusive evolution behavior of the buried solid-solid interfaces is the major barrier to exploring solid-state electrochemical devices. Here, we uncover the interfacial void evolution principles in solid-state batteries, build a solid-state void nucleation and growth model, and make an analogy with the bubble formation in liquid phases. In solid-state lithium metal batteries, the lithium stripping–induced interfacial void formation determines the morphological instabilities that result in battery failure. The void-induced contact loss processes are quantified in a phase diagram under wide current densities ranging from 1.0 to 10.0 milliamperes per square centimeter by rational electrochemistry calculations. The in situ–visualized morphological evolutions reveal the microscopic features of void defects under different stripping circumstances. The electrochemical-morphological relationship helps to elucidate the current density– and areal capacity–dependent void nucleation and growth mechanisms, which affords fresh insights on understanding and designing solid-solid interfaces for advanced solid-state batteries.
24 September 2025 in Nature
20 August 2021 in Small Science
Lithium–sulfur (Li–S) batteries are highly considered for next‐generation energy storage due to their ultrahigh theoretical energy density of 2600 Wh kg−1. The conversion reactions between lithium polysulfides (LiPSs) constitute the core process in working Li–S batteries. Electrochemical impedance spectroscopy (EIS) analysis of LiPS symmetric cells is an effective tool to provide detailed information on the LiPS conversion reactions and direct further kinetic promotion. However, reasonable interpretation of the EIS responses is so far insufficiently addressed without a well‐defined equivalent circuit. Herein, a systematic analysis on the EIS responses of LiPS symmetric cells is conducted to provide a comprehensible equivalent circuit. Interfacial contact, surface reaction, and diffusion are decoupled according to their respective characteristic frequency using the distribution of relaxation time analysis method. A well‐defined equivalent circuit is proposed to accurately fit the experimental EIS responses, unambiguously interpret key parameters, and be feasible with a wide range of experimental conditions. This work presents the methodology of understanding the EIS responses of LiPS symmetric cells and inspires analogous analysis on vital electrochemical processes.
1 April 2023 in Transactions of Tianjin University
With the increasing scale of energy storage, it is urgently demanding for further advancements on battery technologies in terms of energy density, cost, cycle life and safety. The development of lithium-ion batteries (LIBs) not only relies on electrodes, but also the functional electrolyte systems to achieve controllable formation of solid electrolyte interphase and high ionic conductivity. In order to satisfy the needs of higher energy density, high-voltage (> 4.3 V) cathodes such as Li-rich layered compounds, olivine LiNiPO4, spinel LiNi0.5Mn1.5O4 have been extensively studied. However, high-voltage cathode-based LIBs fade rapidly mainly owing to the anodic decomposition of electrolytes, gradually thickening of interfacial passivation layer and vast irreversible capacity loss, hence encountering huge obstacle toward practical applications. To tackle this roadblock, substantial progress has been made toward oxidation-resistant electrolytes to block its side reaction with high-voltage cathodes. In this review, we discuss degradation mechanisms of electrolytes at electrolyte/cathode interface and ideal requirements of electrolytes for high-voltage cathode, as well as summarize recent advances of oxidation-resistant electrolyte optimization mainly from solvents and additives. With these insights, it is anticipated that development of liquid electrolyte tolerable to high-voltage cathode will boost the large-scale practical applications of high-voltage cathode-based LIBs.