We report a new InP/GaAsSb double heterojunction bipolar transistor (DHBT) emitter fin architecture with a record ${f}_{\mathrm {MAX}} =1.2$ THz, a simultaneous ${f}_{\mathrm {T}} =475$ GHz, and $BV_{\mathrm {CEO}} =5.4$ V. The resulting $BV_{\mathrm {CEO}}\,\times \,{f}_{\mathrm {MAX}} =6.48$ THz-V is unparalleled in semiconductor technology. Devices were realized with a 20-nm-thick compositionally and impurity graded GaAsSb-base and a 125-nm InP collector. The performance arises because the process allows: 1) a tunable base–emitter access distance down to 10 nm; 2) the use of thicker base contact metals; and 3) the minimization of parasitic capacitances and resistances via precise lateral wet etching of the base–collector (B/C) mesa. Perhaps more significantly, InP/GaAsSb DHBTs with ${f}_{\mathrm {MAX}} \ge1$ THz are demonstrated with emitter lengths as long as 9.4 $\mu \text{m}$ and areas as high as 1.645 $\mu \text{m}$ 2 . Such an area is > $6\times $ larger than previously reported terahertz (THz) DHBTs, representing a breakthrough in THz transistor scalability. This attractive performance level is achieved with a very low dissipated power density which makes InP/GaAsSb DHBTs well-suited for high-efficiency millimeter- and submillimeter-wave applications. Furthermore, we provide the first large-signal characterization of a THz transistor with 94 GHz load-pull measurements showing a peak power-added-efficiency (PAE) of 32.5% (40% collector efficiency) and a maximum saturated power of 6.67 mW/ $\mu \text{m}$ 2 or 1.17 mW/ $\mu \text{m}$ of emitter length in a common-emitter configuration. Devices operate stably under large-signal conditions, with voltages nearly twice higher than those for peak small-signal performance.
7 September 2017 in IEEE Transactions on Semiconductor Manufacturing
A Pt/Ti/Pt/Au gate electrode stack is commonly used in AlInAs/GaInAs/InP high electron mobility transistors (HEMTs) due to the high Schottky barrier height of Pt on AlInAs and the fact that Pt can be controllably diffused through semiconductor layers thereby enabling vertical scaling. We show here that the Pt-AlInAs reaction is not only controlled by the annealing time and temperature — the annealing ambient and the thermal ramp rate also affect the diffusion of Pt through the underlying semiconductor layers and impact the DC and RF device performance. Following the gate metal deposition, one process split was rapid thermal annealed (RTA) at 250°C and subsequently passivated by atomic layer deposition (ALD) at 180°C. For the second process split, the Pt gate sink-in process was carried out in the ALD system at 250°C simultaneously with the gate passivation. Despite identical gate sink-in temperatures, the two process splits exhibit different characteristics suggesting different gate-to-channel distances. The distance of the Pt gate to the GaInAs channel was therefore confirmed through high-resolution cross-sectional scanning transmission electron microscopy (STEM) analysis. The results presented here reveal that both the suitable ramp rate and the sink-in ambient are necessary to achieve a fully sunken Pt gate.
2 October 2019 in IEEE Transactions on Electron Devices
GaInAs/InAs composite channels in InP-based pHEMTs enable wideband and/or low-noise performances because of their superior carrier transport properties. To date, the influence of the InAs inset design details on transistor performance has not been parametrized in the literature. We present a systematic study of the effects of the InAs channel inset thickness on transistor characteristics and cutoff frequencies versus temperature, and on the noise performance at 300 K. The epitaxial layer structures considered here incorporate 2 to 5-nm InAs insets in a fixed total composite channel thickness. All layers exhibit excellent electron mobilities (from 40,200 to 54,800 cm²/Vs at 77 K). Thicker InAs insets improve both the current gain cutoff frequency (fT) and the maximum oscillation frequency (fMAX). However, they also result in higher gate leakage currents and increased channel impact ionization. 50-nm gate length pHEMTs with a 5-nm InAs inset feature the highest simultaneous fT/fMAX ≥ 390/675 (455/800) GHz at 300 (15) K for a low-noise bias but exhibit the poorest minimum noise figure NFMIN. Whereas higher fT (and/or fMAX) values have traditionally been associated with improved noise performances, this is no longer the case.
GaInAs-based Metal Oxide Semiconductor High Electron Mobility Transistors (MOS-HEMTs) can in principle combine the wide bandwidth of HEMTs to the low gate leakage current of MOSFETs in a single deeply-scaled ultrahigh speed low-noise technology. Despite advances in the fabrication of MOS-HEMT devices and MMICs, the transistor microwave noise properties of GaInAs MOS-HEMT devices have not yet been reported. In the present study, the room temperature DC and wideband RF noise properties (8-50 GHz) of GaInAs channel MOS-HEMTs are characterized and contrasted to those of a 50 nm low-noise HEMT with the same channel composition/thickness and similar fT: at a given bias VDS = 0.5 V, the HEMT provides lower minimal noise figures (NFMIN) and higher associated gain. In contrast to HEMTs, the MOS-HEMTs particularly suffer from lower frequency noise contributions attributed to enhanced impact ionization. Remarkably, operation at VDS = 0.4 V to mitigate ionization enables MOS-HEMTs to match the HEMT wideband NFMIN performance despite a significantly poorer low-field channel mobility. The present MOS-HEMTs show the highest reported maximum oscillation frequency fMAX = 637 GHz for a measured gate length LG = 33 nm and a (2 × 15) μm width. Gate annealing is shown to be deleterious to the MOS-HEMT DC and noise properties.
10 September 2019 in IEEE Transactions on Semiconductor Manufacturing
Optimum device performance in terms of noise and gain of AlInAs/GaInAs/InP High Electron Mobility Transistors (HEMTs) requires minimizing the contact resistance RC. In several HEMT fabrication steps in device manufacturing it is common to expose highly-doped semiconductors layers to heated solvents for prolonged periods of time. It is shown here that even a small amount of water or water vapor present during photoresist removals, metal lift-offs or related processes can dramatically affect the final device performance by promoting electrochemical etching of the semiconductor layers adjacent to metal stacks. In this paper, the impact of metal lift-off on erosion of HEMT epitaxial layers and Ohmic contact resistance is studied with respect to different layer doping levels, compositions and metal stacks forming the Ohmic contacts.