1 June 2018 in Materials Science Forum
As part of a study devoted to the effect of trace elements on graphite degeneracy, near-eutectic ductile iron melts were prepared to which minute amounts of lead and of both lead and cerium were added. The melts were cast into an insulated Y4 mould, giving a solidification time of about 1 hour and a cooling time to room temperature of about 15 hours. In the thermal centre of the Pb containing sample graphite spheroids as well as intergranular lamellar graphite have been found. At the same location of the casting containing both Pb and Ce, exploded as well as chunky graphite could be observed, while the formation of intergranular lamellar graphite has been suppressed. Deep etching of the samples allowed reaching the following conclusions: i) intergranular graphite in the SG-Pb sample often, if not always, originates on graphite nodules and extends towards the last to freeze areas; ii) in one location of the SG-PbCe sample, chunky graphite strings were observed to originate on an exploded nodule, thus confirming the close relationship between these two forms of graphite. Because of the over-treatment in cerium of the SG-PbCe sample, other unusual degenerate graphite was observed which appears as coarse aggregates of "porous" graphite after deep etching.
25 February 2020 in International Journal of Metalcasting
Antimony is used in ductile cast iron melts to avoid graphite degenerations like exploded graphite and chunky graphite. However, the effect of Sb in the melt on the crystallization of ductile cast iron is still unknown, therefore the aim of our investigations. The current study presents thermodynamic calculations showing that at the beginning of the eutectic solidification, Mg3Sb2 is formed. Furthermore, the amount of Sb increases in the austenite and decreases in the remaining melt during solidification. An experiment was conducted, in which a higher amount of Sb than usual was added to a ductile iron melt. In the microstructure of the Sb-containing sample, a higher graphite precipitate count was measured than in the reference sample without Sb. The graphite spheroids of the Sb-containing sample show an almost perfect roundness and a very smooth surface. However, lamellar outgrowths from the graphite spheroids were also observed. Using scanning electron microscopy with energy-dispersive X-ray spectroscopy, it could be shown that Sb-containing phases have been formed, which are located in the pearlitic matrix and also in graphite spheroids. As a result of spectroscopic investigations, it can be assumed that Sb-containing phases act as nucleant for graphite nucleation. Further investigations by Auger electron spectroscopy showed that a thin layer of Sb at the interface between graphite and matrix has been formed. It seems that this layer constricts the diffusion of carbon to the spheroidal graphite and acts as a surfactant favoring a layer-by-layer growth of the graphite spheroids.
4 September 2022 in International Journal of Metalcasting
The impact of combined addition of high levels of bismuth up to 120 wt ppm and cerium up to 2000 wt ppm on the graphite morphology in GJS 450-18 with 3.2 wt% carbon and 3.2 wt% silicon was studied. Experiments were conducted with insulated keel blocks with a solidification time of 40 min. Samples from the thermal centre of the castings were analysed by optical microscopy, and the forms and sizes of graphite particles were characterised. Bismuth addition, even at 25 wt ppm, resulted in an altered graphite form in the last-to-freeze regions resembling intercellular lamellar graphite (ILG). Additions of 45 wt ppm or more Ce to these Bi-containing melts prevented the formation of ILG and produced chunky graphite (CHG) instead. ILG did not appear for ratios Bi/Ce > 1.5, while CHG could not be found for ratios Bi/Ce < 0.7. Only one type of graphite degeneration (either ILG or CHG) was present in each sample, thus rendering their formation mutually exclusive. Larger amounts of Ce between 300 and 500 wt ppm resulted in the formation of predominantly graphite form V, while no degenerations could be observed. The addition of Ce to a Bi-contaminated cast iron melt to avoid ILG formation and achieve a regular graphite structure with mainly form VI graphite is not possible. Instead, form V replaces form VI as the predominantly formed morphology. Ce levels higher than 1000 wt ppm resulted in the formation of large areas of undercooled graphite in the last-to-freeze regions regardless of the Bi content in the cast iron melt.
27 December 2023 in International Journal of Metalcasting
The mechanical properties of ausferritic ductile iron are strongly influenced by the ability of the austenite to undergo martensite formation. Strain-induced martensite formation occurring under the right circumstances results in transformation induced plasticity (TRIP) that improves ductility and strength. TRIP has been shown to depend on the austenite’s stacking fault energy (SFE), which describes the crystals micromechanical behaviour. In austenitic FeMnAlSi-TRIP steels, TRIP as a reaction to mechanical load only occurs for SFE <20 mJ/m2. For carbon-stabilised austenite as in ADI, the relationship between stacking faults, mechanical properties and martensitic transformation has not yet been established. To investigate the TRIP-effect in ADI, unalloyed ADI with 3.43 wt% C, 2.52 wt% Si and 0.21 wt% Mn was ausferritised and subjected to tensile tests at temperatures between −180 °C and 200 °C. The amount of martensite produced by thermal and mechanical activation, crystalline microstrain and stacking fault density were measured on deformed and undeformed regions of the specimen by XRD and the resulting SFE calculated. Between −70 and 20 °C, the elongation at fracture exceeded 10 % compared to below 2 % in the temperature range of −130 to −180 °C. At temperatures above 80 °C, elongation at fracture gradually decreased to 4.5 % at 200 °C. High sample ductility was associated with lower SFEs as low as 35 mJ/m2, indicating a correlation of stacking fault formation and strain-induced martensite formation in ADI.
29 January 2024 in International Journal of Metalcasting
Heavy section Austempered Ductile Iron (ADI) components may contain pearlitic or a mixed microstructure (mixture of pearlite and ausferrite) in their centres besides ausferrite. As a result, mechanical properties are not homogeneously distributed across the thicknesses of the components. The oversizing of the components therefore leads to unnecessary material expenses in foundries. In order to avoid the complex manufacturing process of heavy section ADI components and subsequent investigations, preliminary tests were performed with smaller test samples. Here, temperature-time curves were detected during heat treatment at different depths. Material samples of the customised composition were heat treated in a dilatometer under the same heat treatment conditions according to different sections of the cast component. A variation of the quenching rates was conducted to investigate the influence on the mixed microstructure formation and ratio of pearlitic and ausferritic microstructures. A comparison of the conventionally heat-treated and dilatometer produced microstructures proved the successful application for heavy section parts and enables microstructure predictions with small samples only. In this way, there is no requirement of expensive tests with high-mass components.
10 February 2016 in International Journal of Cast Metals Research
In nodular cast iron, molybdenum is alloyed in the range of 0.5 to 1.5 wt.-% to increase the mechanical properties for high temperature application, especially for thick walled castings like housings of gas or steam turbines. The behaviour of Mo precipitates in the as cast state as well as under long exposure to heat was the object of this investigation. In the as cast state, Mo forms metastable carbidic grain boundary precipitates with iron, silicon and carbon. These transform into stable MoC precipitates during sustained temperature influence. Furthermore, there are finely dispersed Mo containing precipitates found in the matrix. These increase the high temperature strength of Mo alloyed cast iron due to the Orowan mechanism and the occurrence of additional grain boundaries. However, it has been shown that these Mo containing precipitates underlie Ostwald ripening under continuous heat exposure, and a precipitate free area occurs along the ferritic grain boundary.