10 December 2024 in Journal of Physics D: Applied Physics
Anode activity in high current vacuum arcs leads to the formation of various high current modes and transitions between them. Intense material evaporation during the anode spot mode and formation of a neutral vapour cloud during the anode plume mode modify the arc plasma properties and, hence, can have a crucial impact in applications, like e.g. reduction of interruption performance of switching devices. The influence of anode mode appearance on arc plasma parameters and on anode surface temperature was studied in detail by a novel optical diagnostic technique—intensified video optical emission spectroscopy. Employing advanced diagnostic methods, the ground state density, excitation temperature and pressure profiles close to the anode surface have been determined. For the anode plume mode, higher copper vapour pressure was found in the plume shell compared to its core. The copper ion density distribution shows a maximum outside of the plume shell. Consequently, a higher electrical conductivity in the surrounding area of the plume might be expected, i.e. the arc current flows around the plume rather than through it. Analysis of the temporal evolution of electrical and optical signals reveals that voltage jumps and drops during the mode transitions are accompanied by noticeable changes in the anode surface temperature. Thus, the formation of the anode plume leads to temperature lowering while the transition to the anode spot mode is accompanied by a temperature increase. In general, a clear correlation between electrode surface temperature and arc voltage in the case of constricted anode attachment is found. The results of this study give new insights into anode plume properties and consequences of anode mode transitions. Reversible mode transitions and correlations between arc voltage and anode surface temperature, as well as changes in the current path during anode plume mode, have to be considered as factors for optimization of electrode design and choice of materials for switching applications.
24 February 2022 in IEEE Transactions on Power Delivery
Replacing SF6, the most potent greenhouse gas, with an alternative is a challenge that medium-voltage load break switch (MV-LBS) has faced. Air is a possible alternative, but there are some challenges regarding low dielectric strength leading to high arcing time and dissipated energy. Therefore, understanding the switching operations in air MV-LBS is crucial to design efficient compact switchgear. This work focuses on making operations in air MV-LBS. A synthetic test circuit and a model switch are designed based on the standards to simulate making operations under fault conditions similar to a real test. The test condition is set to achieve high pre-strike arcing time and energy. The results show that the most destructive impact of the making short-circuit current occurs in the first half-cycle of the load current when the pre-strike arc is formed. With an average short-circuit current with a peak of 22 kA and a breakdown voltage of 20 kV, the switch failed to re-open due to the arcing contacts welding after four successive making operations without main contacts and seven successive operations with main contacts. It has been shown that the total arcing contact mass loss occurs mainly during the pre-arcing time.
9 April 2021 in Journal of Physics D: Applied Physics
Medium voltage load break switches (MV-LBS) should pass fault current while closing and be able to re-open for the next operation. Replacing SF 6 as a high impact greenhouse insulating gas with air, makes the switch design more challenging because of the higher pre-strike arcing time and energy dissipation between contacts which leads to more contact surface erosion and an even higher possibility of welding. In this paper, a synthetic test circuit is used to emulate stresses applied to MV-LBS during the making of short-circuit currents. Since there are difficulties in accurate direct measurement of arc voltage because of the inherent response of the measurement system, an alternative method using optical emission spectroscopy (OES) is proposed. OES measures the pre-strike arc temperature distribution profile close to the cathode surface at a test voltage of 18 kV and a making current of 17 kA. The arc electrical characterization is achieved using the obtained spectroscopy results, Lowke’s model and thermal air plasma transport properties. A maximum arc temperature of 12 500 K while the arc moves from the lower part of the cathode to the center, arc voltage of 30–58 V, and dissipated energy of 79–87 J are calculated for the pre-strike arc considering the impact of copper evaporated from the contact surfaces. Different arc behavior is observed in closing the contacts compared to free-burning arcs, which indicates gas flow blowing the arc caused by the contact movement. This investigation could be used for a better understanding of switching behavior and efficient control of the operation.
23 September 2020 in IEEE Transactions on Plasma Science
Energy dissipation during prestrike arc is the critical factor for electrical contacts erosion and welding in medium voltage load break switches. Using air-filled devices as an alternative to SF₆ makes the switch environmentally friendly, but leads to a more challenging process due to a higher prestrike arcing time between contacts. Therefore, understanding the erosion process of electrical contacts is crucial to improve the switch lifetime. Determination of contacts surface evaporation by optical emission spectroscopy is one of the most precise methods to investigate the prestrike arc interface with the contacts. In this article, the temporal and spatial profiles of copper and tungsten emitted species during prestrike arc are presented. For this purpose, a circuit consisting of a synthetic dc high voltage part is used to initiate the arc. The temporal evolution of CuI, CuII, and WI shows evaporation of the cathode and the anode surfaces during the prestrike arc, and the spatial profiles show an inhomogeneous distribution of the vapors alongside the arc root.
16 July 2024 in Measurement Science and Technology
Switching arc characterization, e.g. measuring the arc voltage and current, is crucial for assessing the performance of power switchgears under different working conditions. This is especially challenging for short circuit current making as one of the most severe operations for medium voltage load break switches. By closing the switch, a short circuit current flows through the arc which is ignited by the electrical breakdown in the gap between contacts before the contacts touch. This results in an abrupt change from the rated voltage of the power network, i.e. tens of thousands of volts, to the switching arc voltage, i.e. a few tens of volts and ultimately zero when the contacts touch. The inherent response of the measurement system to this very large step preceding the arc formation overlaps with the switching arc voltage and results in unrealistic arc voltages which makes correction of the distorted voltage waveform necessary. In this paper, a post processing method based on deconvolution correction technique, i.e. deconvolution of the measured voltage in time and frequency domains, is examined using experimentally determined impulse responses of the measurement system. To demonstrate its effectiveness, this method is applied to three different measurement system configurations with various step responses. The results show practically identical deconvoluted (corrected) voltage waveforms in all three measurement systems, although the directly measured waveforms have significant differences. The corrected arc voltage waveforms are in agreement with the indirect measurements proposed in previous studies.