1 March 2017 in Journal of Environmental Radioactivity
The main goal of research presented in this paper was the material and radiological characterization of high volume fly ash concrete (HVFAC) in terms of determination of natural radionuclide content and radon emanation and exhalation coefficients. All concrete samples were made with a fly ash content between 50% and 70% of the total amount of cementitious materials from one coal burning power plant in Serbia. Physical (fresh and hardened concrete density) and mechanical properties (compressive strength, splitting tensile strength and modulus of elasticity) of concrete were tested. The radionuclide content (226Ra, 232Th and 40K) and radon massic exhalation of HVFAC samples were determined using gamma spectrometry. Determination of massic exhalation rates of HVFAC and its components using radon accumulation chamber techniques combined with a radon monitor was performed. The results show a beneficial effect of pozzolanic activity since the increase in fly ash content resulted in an increase in compressive strength of HVFAC by approximately 20% for the same mass of cement used in the mixtures. On the basis of the obtained radionuclide content of concrete components the I -indices of different HVFAC samples were calculated and compared with measured values (0.27-0.32), which were significantly below the recommended 1.0 index value. The prediction was relatively close to the measured values as the ratio between the calculated and measured I-index ranged between 0.89 and 1.14. Collected results of mechanical and radiological properties and performed calculations clearly prove that all 10 designed concretes with a certain type of fly ash are suitable for structural and non-structural applications both from a material and radiological point of view.
1 April 2019 in Science of The Total Environment
Poor storage of industrial wastes has been a cause of land contamination issues. These wastes or by-products have the potential to be used as secondary raw materials in construction, promoting the concept of a circular economy that will avoid land contamination. Here we evaluate radiological environmental impacts when wastes that contain elevated levels of naturally occurring radionuclides (NORs) such as red mud, fly ash and ground granulated blast furnace slag are made into 'green cements' such as geopolymers or alkali-activated materials (AAMs). During the study, three AAM concrete and mortar series with various mixing ratios were prepared and investigated. The NOR content, I-Index, radon emanation and exhalation of the precursor waste materials and their cement products were measured and calculated and the strength of the cement products was compared. The emanation and the exhalation properties were calculated for the final products, weighing the data of the components as a function of their mixing ratio. The I-index alone suggested that the AAMs would be suitable products. AAMs containing ground granulated blast furnace slag exhibited the lowest radon exhalation and higher compressive strength, while the fly ash and red mud AAMs had increased final radon exhalation. In the case of fly ash, alkaline activation of fly ash dramatically increased the radon exhalation; the highest measured fly ash exhalation was 1.49 times of the theoretically calculated exhalation value. This highlights the increased risk of using fly ash as a component in AAMs and the need to carry out testing on the final products as well as individual secondary raw materials.
1 October 2015 in Journal of Environmental Radioactivity
The reuse of industrial by-products is important for members of numerous industrial sectors. However, though the benefits of reuse are evident from an economical point of view, some compounds in these materials can have a negative effect on users' health. In this study, the radon emanation and exhalation features of red mud were surveyed using heat-treatment (100-1200 °C). As a result of the 1200°C-treated samples, massic radon exhalation capacity reduced from 75 ± 10 mBq kg(-1) h(-1) to 7 ± 4 mBq kg(-1) h(-1), approximately 10% of the initial exhalation rate. To find an explanation for internal structural changes, the porosity features of the heat-treated samples were also investigated. It was found that the cumulative pore volume reduced significantly in less than 100 nm, which can explain the reduced massic exhalation capacity in the high temperature treated range mentioned above. SEM snapshots were taken of the surfaces of the samples as visual evidence for superficial morphological changes. It was found that the surface of the high temperature treated samples had changed, proving the decrement of open pores on the surface.
1 March 2017 in Journal of Environmental Radioactivity
1 January 2018 in Construction and Building Materials
1 September 2017 in Construction and Building Materials