The new R&D programme of JAEA/CLADS tests complements the previous investigations related to BWR severe accidents. A series of tests aim at closing the gaps in understanding of the Fukushima Dai-Ichi degradation sequence at each unit. The paper emphasises the problem of control blade degradation, which influences the accident progression at an early stage and shows the approach for thorough investigation of this problem.
9 December 2020 in Journal of Nuclear Science and Technology
In February 2019, TEPCO and TOSHIBA designed a robot that can handle the debris, performed a trial investigation of primary containment vessel (PCV) of the Fukushima Dai-Ichi (1F) Unit 2 and published a video. The video contained lots of valuable information which can be compared with results of BWR control blade degradation tests recently performed in Japan Atomic Energy Agency (JAEA). During the test under postulated 1F Unit 2 simulated conditions a complex behaviour of the test sample with the formation of mostly three types of debris was observed. Possible mechanisms governing the 1F Unit 2 debris formation and possible ways of their relocation are discussed.
The article studies dependences of grain size in Ni3Al intermetallic compound synthesized under pressure in 3Ni+Al powder mixture in conditions of bulk exothermal reaction upon pre-pressure acting on the powder mixture and upon a delay time of applying pressure to a high-temperature synthesis product. It is proved that an increase in the pre-pressure on the parent powder mixture reduces the grain size, and an increase in the delay time increases the grain size in the synthesized intermetallic compound. Reducing the grain size from 10 to 1.75μm increases the strength of the intermetallic compound under pressure from 336 to 482 MPa (1.4 times).