Shuang-Zhang Wu

Shuang-Zhang Wu

Auto-generated profile, based on publicly available information

Shuang-Zhang Wu

College of Field Engineering

Research Focus & Metrics

Academic Career Length

11Years (2016-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 January 2018 in Advances in Materials Science and Engineering
Verified
Journal Article
Open access
PDF file
JWJiaxiang Wu
Jiaxiang Wu
XFXiang Fang
Xiang Fang
ZGZhen-Ru Gao
Zhen-Ru Gao
HWHuai-Xi Wang
Huai-Xi Wang
JHJunyi HUANG
Junyi HUANG
YLYuchun Li
Yuchun Li
Al‐PTFE (aluminum‐polytetrafluoroethylene) serves as one among the most promising reactive materials (RMs). In this work, six types of Al‐PTFE composites with different Al particle sizes (i.e., 50 nm, 1∼2 μm, 6∼7 μm, 12∼14 μm, 22∼24 μm, and 32∼34 μm) were prepared, and quasistatic compression and drop weight tests were conducted to characterize the mechanical properties and reaction characteristics of Al‐PTFE composites. The reaction phenomenon and stress‐strain curves were recorded by a high‐speed camera and universal testing machine. The microstructure of selected specimens was anatomized through adopting a scanning electron microscope (SEM) to correlate the mesoscale structural characteristics to their macroproperties. As the results indicated, in the case of quasistatic compression, the strength of the composites was decreased (the yield strength falling from 22.7 MPa to 13.6 MPa and the hardening modulus declining from 33.3 MPa to 25 MPa) with the increase of the Al particle size. The toughness rose firstly and subsequently decreased and peaked as 116.42 MJ/m3 at 6∼7 μm. The reaction phenomenon occurred only in composites with the Al particle size less than 10 μm. In drop weight tests, six types of specimens were overall reacted. As the Al particle size rose, the ignition energy of the composites enhanced and the composites turned out to be more insensitive to reaction. In a lower strain rate range (10−2·s−1∼102·s−1), Al‐PTFE specimens take on different mechanical properties and reaction characteristics in the case of different strain rates. The formation of circumferential open cracks is deemed as a prerequisite for Al‐PTFE specimens to go through a reaction.

20 December 2016 in Central European Journal of Energetic Materials
Verified
Journal Article
Open access
FBFeng Bin
Feng Bin
XFXiang Fang
Xiang Fang
YLYuchun Li
Yuchun Li
SWShuang-Zhang Wu
Shuang-Zhang Wu
YMYi-Ming Mao
Yi-Ming Mao
HWHuai-Xi Wang
Huai-Xi Wang