1 March 2020 in Journal of Physics: Conference Series
Crushing and grinding are widely used in mining, mineral processing, cement making, and coal power generation. The mechanical components that contact with materials being processed are working under the conditions of high abrasion and impact. How to reduce the wearing damages and prevent from the cracking failure of the mechanical parts is one of the crucial challenges facing the operations of many industries, involved crushing and grinding processes. Whit cast irons, and specifically high chromium white cast irons, have been developed and deployed worldwide for making mechanical components of crushing and grinding machines due to the combination of high wear resistance and good mechanical strength. The paper is aimed to give an overview on the white cast iron alloys, and particularly high chromium white cast iron alloys, including their classifications, their standard specifications in USA, China and Australia, their main usages and the new developments.
23 July 2021 in Energy & Fuels
1 January 2017 in AIP Conference Proceedings
Austenitic manganese steel has a high toughness, high ductility, high strain hardening capacity and excellent wear resistance, the material is mostly used in the mining industry for crushing and loading equipment. High manganese steel shows superior wear resistance when used under primary crushing system than when used under secondary and tertiary modes of crushing. This work presents the effect of vanadium content on the mechanical properties and microstructure evaluation of high manganese steel. The addition of vanadium to high manganese steels has a direct increase on the hardness and wear resistance. Impact testing for alloys containing vanadium showed low impact energies compared to the standard manganese steel. The increase in hardness and the wear resistance of the alloys was explained based on the vanadium carbide which had formed on the austenitic matrix. It was observed that the carbon and vanadium content will influence the mechanical properties of high manganese steel alloyed with vanadium. Microstructural examination showed that the size and distribution of vanadium carbidesinfluences the mechanical properties and the wear behaviour. Therefore, this work showsthat the addition of vanadium to high manganese steel will increase the hardness and wear resistance while decreasing the impact energy of high manganese steel alloyed with vanadium.
23 June 2015 in Journal of Energy in Southern Africa
Energy efficiency is nowadays one of the biggest concerns worldwide. It has become one of the critical matters to any country and industry particularly in South Africa. Because of the complexities and challenges found in industries and especially in foundry, many strategies have been established to measure and regulate more efficiently the energy. Many studies have been conducted in steelmaking process and electrical arc furnace using foaming slag to reduce energy consumption. As such, in this case study, the experiment will be conducted in a small foundry metal casting laboratory using an Induction Furnace (IF), which will reduce energy usage by using the foaming slag and as well pointing out the importance and the impact of carbon rate change on the foaming creation. After experiments all results show that the melting time can be reduced from 42min to 35 min, which is 20% time saving, the electrical energy consumption also has been reduced from 13.93kWh to 10kWh which is 39.3% saving. On the other hand, the foaming slag optimum height was reached at 1 cm. Therefore, a simple modelling has been designed and calculations have been made on heat transfer at the surface opening of the Induction Furnace and temperature loss has been reduced from 878°C to 870°C, with heat transfer loss reduced from 27.99kW to 26.38kW which was 6.10% of energy saving.
1 March 2020 in Journal of Physics: Conference Series
High chromium white cast irons (HCWCI) are widely used as abrasion resistant materials in cement manufacturing, mineral processing and slurry pumping industries. Their high resistance to wear in these demanding situations stems from the presence of hard eutectic (Cr, Fe)7C3 carbides in their microstructures. In this context, the properties of hypoeutectic iron of HCWCI containing 25 wt. %Cr-2.5 wt. %C were investigated after destabilisation heat treatments, cooling (slow and fast cooling) to ambient temperatures, their influence on the microstructure was investigated. For characterization of the hypoeutectic iron of HCWCI, several experimental tests were performed using the following laboratory equipment: light optical microscope, scanning electron microscope. The amount of retained austenite also depends on the alloying additions in the melt during melting processes, destabilisation temperatures, soaking time and the cooling rates during heat treatment processes.
1 January 2013 in IFAC Proceedings Volumes