Ruslan E. Nikolaev

Ruslan E. Nikolaev

Auto-generated profile, based on publicly available information

Ruslan E. Nikolaev

Novosibirsk State University, 1, Pirogova str., Novosibirsk, 630090, Russia

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
30 May 2023 in Optical Materials
Verified
Journal Article
Closed access
VPVladimir Pustovarov
Vladimir Pustovarov
RNR.E. Nikolaev
R.E. Nikolaev
VTV.A. Trifonov
V.A. Trifonov
MTMaria S. Tarasenko
Maria S. Tarasenko
SDS.J. Dhoble
S.J. Dhoble
NNNikolay Naumov
Nikolay Naumov

19 August 2023 in Optical Materials
Verified
Journal Article
Closed access
VPVladimir Pustovarov
Vladimir Pustovarov
IOI.N. Ogorodnikov
I.N. Ogorodnikov
RNR.E. Nikolaev
R.E. Nikolaev
MTMaria S. Tarasenko
Maria S. Tarasenko
DTDmitry A. Tavrunov
Dmitry A. Tavrunov
NNNikolay Naumov
Nikolay Naumov

24 December 2021 in CrystEngComm
Verified
Journal Article
Closed access
PDF file
IVInga G. Vasilyeva
Inga G. Vasilyeva
RNRuslan E. Nikolaev
Ruslan E. Nikolaev
Advances and limitations in the field of growing large, high optical quality single crystals of AgGaS 2 (AGS), AgGaGeS 4 (AGGS), ZnGeP 2 (ZGP), LiInS 2 (LIS), LiGaS 2 (LGS), LiInSe 2 (LISe), LiGaSe 2 (LGSe) and LiGaTe 2 (LGT) are considered in this article.

30 August 2019 in CrystEngComm
Verified
Journal Article
Closed access
PDF file
IVInga G. Vasilyeva
Inga G. Vasilyeva
RNRuslan E. Nikolaev
Ruslan E. Nikolaev
SNSergei G. Nasonov
Sergei G. Nasonov
AKAlexandr V. Kurchev
Alexandr V. Kurchev
VSVladimir N. Shlegel
Vladimir N. Shlegel
200 g ZnMoO4 single crystals, both pure and doped with WO3, were grown from appropriate powder mixtures of oxides via the low-temperature gradient Czochralski technique, and plates cut from them were characterized in detail. The crystal-chemical formulas of non-stoichiometric Zn1.010ZnyMo1−yO1.010+3−2y (y = 0.007) crystals, being substitutional solid solutions with ionic defects, such as ZnMo 4−, VO 2+, and Zni 2′ , were established based on determination of the compositions, densities and lattice unit cell parameters with very high accuracy. This characterization allowed for clarification of the role played by each stage of crystal growth, including solid-phase powder synthesis, high-temperature homogenization and crystallization, which proceeded sequentially in one reactor that was semi-open to the air. It was shown that MoO3 volatility is the primary source of issues. The first stage, resulting in a non-equilibrium grain-zoning product, was the key to creating MoO3 vapor pressure in the reactor and a melt composition enriched by the ZnO component. The conditions for the stable crystallization of nonstoichiometric crystals were determined. The experimentally observed shifts in the characteristic liquidus and solidus temperatures of non-stoichiometric ZnMoO4 crystals doped by WO3 were found to be of importance to minimize the negative effects of peritectic melting.

3 March 2025 in Journal of Analytical Atomic Spectrometry
Verified
Journal Article
Closed access
PDF file
SNSofia I. Nagornaya
Sofia I. Nagornaya
EPEvgeniya Polyakova
Evgeniya Polyakova
RNRuslan E. Nikolaev
Ruslan E. Nikolaev
ENElena N. Nigmatulina
Elena N. Nigmatulina
The ICP-OES method for determination of the main and trace composition of europium-doped gadolinium(III) oxide crystals from a single solution has been developed. Axial plasma viewing was used for trace analysis, and radial viewing was used for the Eu/Gd determination. Different variants of calibration solution preparation were compared: mixing aliquots and joint dissolution of samples. The parameters of spectra registration that minimized the relative standard deviation (RSD) of the emission intensities were selected; the results obtained using the “aliquot mixing” method coincided with the results of an electron microprobe analysis. The RSD in the Eu/Gd molar ratio is 1.5%. It is shown that the maximum ICP power provides minimum detection limits for trace elements at a Gd concentration of 1500 mg L−1 in solution, amounting to n·10−6 to n·10−3% w/w for 52 elements.

25 January 2021 in CrystEngComm
Verified
Journal Article
Closed access
PDF file
RNR. E. Nikolaev
R. E. Nikolaev
Veronica SulyaevaVeronica Sulyaeva
Veronica Sulyaeva
AAA. V. Alekseev
A. V. Alekseev
ASA. S. Sukhikh
A. S. Sukhikh
EPEvgeniya Polyakova
Evgeniya Polyakova
BNB. Tran Nhu
B. Tran Nhu
The nonequilibrium evaporation of a high-temperature SnS + Dy 2 S 3 solution leads to the implementation of a VLS-like mechanism of growth of γ-Dy 2 S 3 helical single crystals.