The corrosion study of aluminum‐based materials is the topic of a great scientific attention because of increasing the applications in many sectors of these materials. The fluoride ions (F − ) effect on the corrosion behavior of pure aluminum in deaerated 0.05 M sulfuric acid (H 2 SO 4 ) solutions at 25 °C was investigated. The electrochemical measurements such as open circuit potential and potentiodynamic polarization were accomplished to study the effect of fluoride and sulfate ions present in the test solutions. The optical microscopic and atomic force microscopic images were taken to view the morphologies and surface roughness of pure aluminum which coincidence with the corrosion rates found from the immersion of the test specimens using weight loss method. The surface morphology and elemental compositions of pure aluminum was evaluated by scanning electron microscope and energy dispersive X‐ray spectroscopy, respectively. The results showed that the general corrosion was formed on the surface of pure aluminum. It is also revealed that the surface roughness and amount of corrosion of pure aluminum were increased by the presence of even a very small amount of fluoride ions in deaerated sulfuric acid solutions.
The inhibitive effect of methyl-1H-benzotriazole (Me-BTA) on pure aluminum was investigated in fluoride-sulphate media at different sulphate concentrations. The corrosion rate, surface roughness, surface morphology and elemental composition of aluminum were evaluated after 24 h of immersion at 80 ºC in deaerated fluoride-sulphate solutions both with and without Me-BTA. Weight-loss measurements showed that the addition of Me-BTA decreased the corrosion rate of aluminum under the investigated conditions. AFM analysis further revealed a reduction in the surface roughness of the aluminum specimens in the presence of Me-BTA, indicating a less damaged surface after exposure to the aggressive medium. SEM analysis revealed fewer corrosion-related surface products on the Me-BTA-treated specimens than on the uninhibited aluminum. EDX further detected nitrogen and increased carbon content after treatment, consistent with the presence of Me-BTA-derived species on the surface. These surface and elemental changes support the protective role of Me-BTA and the formation of an inhibitor-derived layer on aluminum in the investigated deaerated fluoride-sulphate media.