22 July 2024 in Applied Sciences
Verified
Journal Article
Open access
PDF file
JLJong Sub(Jay) Lee
Jong Sub(Jay) Lee
OKOhsun Kwon
Ohsun Kwon
YHYujoong Hwang
Yujoong Hwang
GYGyumin Yeon
Gyumin Yeon
This study aims to evaluate the tire–road-wear particles (TRWPs) and suspended dust generated based on the nominal maximum aggregate size (NMAS) of the polymer-modified stone mastic asphalt (SMA) mixtures indoors. The SMA mixtures containing styrene butadiene styrene (SBS) polymer and the NMASs of 19, 13, 10, 8, and 6 mm were used. Dust was generated from the wear of the tires and the pavement inside the indoor chamber by using the laboratory tire–road-wear particle generation and evaluation tester (LTRWP tester) developed by Korea Expressway Corporation (KEC). In this method, a cylindrical asphalt-mixture specimen rotates in the center, and a load is applied using three tires on the sides of the test specimen. During the test, a digital sensor was used to measure the concentration for each particle size. After the test was completed, the dust was collected and weighed. According to the test results, the generated TRWP emissions were reduced by approximately 0.15 g as the NMAS of the SMA mixture decreased by 1 mm. TRWP emissions decreased by 20% when using the 6 mm SMA mixture compared to the 13 mm SMA mixture. For practical application, a predicted equation of TRWP emissions estimation was developed by using the concentration of suspended dust measured by the digital sensor in the LTRWP tester. LTRWP can be used as an indoor test method to evaluate pavement and tire materials to reduce the amount of dust generated from tire and pavement wear.

26 August 2024 in Polymers
Verified
Journal Article
Open access
PDF file
JLJong Sub(Jay) Lee
Jong Sub(Jay) Lee
SLSungjin Lee
Sungjin Lee
YHYujoong Hwang
Yujoong Hwang
OKOhsun Kwon
Ohsun Kwon
GYGyumin Yeon
Gyumin Yeon
This study evaluates the crack performance of stone mastic asphalt (SMA) mixtures according to the performance of a modified asphalt binder, evaluated based on the asphalt performance grade (PG) and the elastic recovery of multiple stress creep and recovery (MSCR) according to AASHTO M 320 and T 350. The cracking performance of the mixture was evaluated using the asphalt mixture performance tester (AMPT) according to AASHTO T 378 and T 400 through dynamic modulus and direct tension cyclic fatigue tests. Furthermore, the recently developed viscoelastic continuum damage (VECD) theory was utilized to evaluate the cyclic fatigue index parameter (apparent damage capacity, Sapp) and the permissible heavy vehicle class. For performance evaluation, six modified asphalt mixtures were prepared and tested using SMA aggregate gradation with a nominal maximum aggregate size (NMAS) of 10 mm. The MSCR test results revealed that, of the six asphalt mixtures, the rubber-based PG76-28 exhibited the least initial strain and the highest elastic recovery. The dynamic modulus test results demonstrated that using a rubber-based modifier increased the elastic modulus at high temperatures and decreased it at low temperatures, thereby enhancing resistance to plastic deformation in the summer and reducing low-temperature cracking in the winter. Finally, the correlation between the Sapp performance index and the elastic recovery of modified asphalt and the number of direct tension cyclic loads until failure of the mixture was evaluated as 0.87 and 0.76, respectively.