This study evaluated the corrosion of steel in seawater-mixed concrete with different interfacial transition zones (ITZs) by measuring different corrosion parameters. The ITZs around the steel bars were intentionally varied by applying cement paste coating around the steel bars, which had various water to cement ratios (W/Cs = 0.3, 0.5, and 0.7). Four cases made with slag cement (68% slag) were investigated, including a control case in which no coating was used. To assess macro-cell corrosion current density prism specimens have been made using segmented steel bars. From the casting of the specimens, until they were 30 days old, the current flow was recorded by electrically connecting the segmented steel bars outside the specimens with a data logger. Monitoring of the half-cell potentials throughout steel bars was carried out and measurements of the macro-cell corrosion were completed. Regardless of the specific cases studied, macro-cell corrosion exhibited a consistent trend of decrease. Steel bars having different cement paste coating with low W/Cs improved the ITZs, creating a dense steel-concrete interface that acted as a barrier against chloride ions permeability. However, a cement paste coating with high W/Cs showed more depth of corrosion compared to the control case than the case without coating because of the weak steel-concrete interface.