Nanosheets bearing fluoroalkoxy groups were prepared via exfoliation of a CF3(CF2)7C2H4O derivative of HLaNb2O7·xH2O for application in epoxy-based hybrids.
A systematic study of the film-thickness dependence of soft magnetic properties and magnetization dynamics of Fe73Co25Al2 alloy thin films has been carried out. These films have columnar structures grown along the film normal, with the average width of the columns of about 30 nm. The saturation magnetization Ms is about 1,550 emu/cc, which remains nearly unchanged with film-thickness over a range from 10 to 120 nm. The coercivity Hc is found to increase with film-thickness from 15 to 64 Oe over a range of 11 to about 50 nm, and then slightly decrease with further increase of thickness. The effective damping parameter αeff measured by FMR over a frequency range from 12 to 66 GHz is found to decrease with film-thickness, becoming 0.0004 and 0.0006, for the films deposited onto fused silica and MgO (100) substrate, respectively.
The soft magnetic properties and effective damping parameters of Fe73Co25Al2 alloy thin films are discussed. The effective damping parameter αeff measured by ferromagnetic resonance for the 10 nm-thick sample is nearly constant (≈0.004 ± 0.0008) for a growth temperature Ts from ambient to 200 °C, and then tends to decrease for higher temperatures and αeff is 0.002 ± 0.0004 at Ts = 300 °C. For the 80 nm-thick sample, the αeff seems to increase with Ts from αeff = 0.001 ± 0.0002 at Ts = ambient to αeff = 0.002 ± 0.0004. The αeff is found nearly constant (αeff = 0.004 ± 0.0008) over a temperature range from 10 to 300 K for the 10 nm films with the different Ts (ambient, 100 and 200 °C). Together with an increasing non-linearity of the frequency dependence of the linewidth at low Ts, extrinsic contributions such as two-magnon scattering dominate the observed temperature dependence of effective damping and linewidth.
The dependences of magnetic properties and effective damping parameter (αeff) on film-thickness (d) and growth temperature (Ts) for Fe69Co26Si5 alloy films are investigated. The saturation magnetization (Ms) are found to decrease from approximately 1,700 to 1,500 emu/cm3 with d for Ts = 230 °C. For 40 nm films, the magnetization remains constant over the entire range of Ts from 35 to 360 °C. The coercivity (Hc) values for Ts above 120 °C are approximately 20 Oe. Those films deposited at Ts =120 °C or higher are epitaxial with the relation of FeCoSi//MgO in the film plane. For the films deposited at Ts =230 °C, the αeff rapidly decreases, and then slightly increases with d. The minimum αeff value of 0.002 is obtained at Ts = 230 °C.