With environmental concerns, there is a strong need to develop posterior restorative dental material as a true alternative to dental amalgam, while one of the serious environmental concerns is how to utilize marble waste such as marble dust produced during machining and cutting of stones. Therefore, the present study proposed a material formulation as a solution for both the issues and investigated the performance of silane-treated marble dust-filled dental composite. Fourier Transform Infrared spectroscopy analysis, Raman Spectroscopy analysis, and Thermo-gravimetric analysis were used to characterize treated and untreated filler. The physical and mechanical characterizations such as void content test, water sorption test, micro-hardness, compressive strength test, dynamic mechanical analysis, and thermo-gravimetric analysis were performed. The result of the study indicated that addition of 0–9 wt.% of marble dust powder increased the hardness, compressive strength, and flexural strength in the range of 69–96 HV, 175–296 MPa, and 55–80 MPa, respectively. However, the void content and water sorption were also increased in the range of 0.31–1.41% and 1.05–2.15%, respectively. Further, it was also revealed that dynamic properties and thermal degradation temperature were increased with the increase of marble dust.
This study presents comparative investigation of adding nanohydroxyapatite (HA) (5–20 wt.%) and mineral trioxide aggregate (MTA) (5–20 wt.%) on the physical, mechanical and thermomechanical characterization of dental composite. The performances of both experimental composites were assessed through various physical, mechanical and thermomechanical tests such as void content test, microhardness test, compressive strength test, dynamic mechanical analysis and thermogravimetric analysis. The result of experiment indicated that the addition of 5 wt.% of HA increased the water sorption, hardness and compressive strength by 50.47%, 13.46% and 62.35%, respectively, whereas the addition of 5 wt.% of MTA increased the water sorption, hardness and compressive strength by 19.23%, 100% and 5.44%, respectively. Dynamic mechanical analysis results revealed that the addition of 5 wt.% HA increased the storage modulus by 10.21%, whereas the addition of 5 wt.% of MTA decreased the storage modulus by 11.79%. The filler HA proved to be better choice in term of thermal stability behavior as compare to MTA filler.
5 August 2016 in Proceedings of the Institution of Mechanical Engineers, Part J: Journal of Engineering Tribology
The purpose of this investigation was to analyze the effect of adding different weight fraction of nanozirconia on wear characteristics of resin-based dental composite. The dental composites were fabricated by adding (0–3 wt.%) of silane-modified nanozirconia particles into a monomer system (50 wt.% bisphenol-A glycidyl methacrylate, 49 wt.% tri-ethylene glycol dimethacrylate, 0.2 wt.% Camphorquinone, and 0.8 wt.% ethyl 4 dimethyl amino benzoate). The experiments were conducted based on steady state condition and Taguchi’s orthogonal design in a dental wear simulator. A theoretical model was proposed for wear assessment and validated with the experimental results. The findings of the experiments indicated that the composite with 3 wt.% nanozirconia demonstrated lowest volumetric wear rate.