The lack of efficient water-soluble two-photon absorption (TPA) photoinitiators has been a critical obstruction for three dimensional hydrogel microfabrications with high water load by two-photon induced polymerization (TPIP). In this paper, a series of cyclic benzylidene ketone-based two-photon initiators, containing carboxylic acid sodium salts to improve water solubility, were synthesized via classical aldol condensation reactions. The cytotoxicity of cyclopentanone-based photoinitiators is as low as that of the well-known biocompatible photoinitiator Irgacure 2959 as assessed in the dark with MG63 cell line. In z-scan measurement, the TPA cross sections of the investigated initiators are only moderate in water, while the TPA values for hydrophobic analogues measured in chloroform were much higher. All novel initiators exhibited broad processing windows in TPIP tests using hydrophilic photopolymers with up to 50 wt% of water. Impressively, microfabrication of hydrogels with excellent precision was possible at a writing speed as high as 100 mm s−1.
In this work the formation of laser-induced periodic surface structures (LIPSS) on a titanium surface upon irradiation by linearly polarized femtosecond (fs) laser pulses with a repetition rate of 1 kHz in air environment was studied experimentally. In particular, the dependence of high-spatial-frequency-LIPSS (HSFL) characteristics on various laser parameters: fluence, pulse number, wavelength (800 nm and 400 nm), pulse duration (10 fs – 550 fs), and polarization was studied in detail. In comparison with low-spatial-frequency-LIPSS (LSFL), the HSFL emerge at a much lower fluence with orientation perpendicular to the ridges of the LSFL. It was observed that these two types of LIPSS demonstrate different fluence, shot number and wavelength dependencies, which suggest their origin is different. Therefore, the HSFL formation mechanism cannot be described by the widely accepted interference model developed for describing LSFL formation.
14 June 2011 in Journal of Polymer Science Part A: Polymer Chemistry
In this paper, the influence of the pulse duration on the ablation threshold and the incubation coefficient was investigated for three different types of materials: metal (copper), semiconductor (silicon) and biopolymer (gelatin). Ablation threshold values and the incubation coefficients have been measured for multiple Ti:sapphire laser pulses (3 to 1000 pulses) and for four different pulse durations (10, 30, 250 and 550 fs). The ablation threshold fluence was determined by extrapolation of curves from squared crater diameter versus fluence plots. For copper and silicon, the experiments were conducted in vacuum and for gelatin in air. For all materials, the ablation threshold fluence increases with the pulse duration. For copper, the threshold increases as τ0.05, for silicon as τ0.12 and for gelatin as τ0.22. By extrapolating the curves of the threshold fluence versus number of pulses, the single-shot threshold fluence was determined for each sample. For 30 fs pulses, the single-shot threshold fluences were found to be 0.79, 0.35, and 0.99 J/cm2 and the incubation coefficients were found to be 0.75, 0.83 and 0.68 for copper, silicon and gelatin, respectively.
The dynamics of the laser-ablation (-desorption) process of metals (Al, Ag, Fe, and Ni) initiated by 30 fs laser pulses has been investigated by interferometric time-resolved pump-probe measurements. It is postulated that a sufficiently high density of hot electrons is essential for achieving desorption of metal ions. In addition, we have observed a new and unexpected behavior characterized by delayed ablation for a pump-probe beam delay in the range of several ps for Al, Ni, and Fe. This second peak is attributed to the development of a liquid surface layer developing after a few ps. Molecular dynamics simulations support this assumption.