Bias temperature stress stabilities of thin-film transistors (TFTs) using In–Ga–Zn–O (IGZO) channels prepared by the atomic layer deposition process were investigated with varying channel thicknesses (10 and 6 nm). Even when the IGZO channel thickness was reduced to 6 nm, the device exhibited good characteristics with a high saturation mobility of 15.1 cm2 V−1 s−1 and low sub-threshold swing of 0.12 V dec−1. Excellent positive and negative bias stress stabilities were also obtained. When positive bias temperature stress (PBTS) stability was tested from 40 to 80 °C for 104 s, the threshold voltages (VTH) of the device using the 6 nm-thick IGZO channel shifted negatively, and the VTH shifts increased from −0.5 to −6.9 V with the increasing temperature. Time-dependent PBTS instabilities could be explained by a stretched-exponential equation, representing a charge-trapping mechanism.
Biological synaptic behaviors such as short-/long-term plasticity were implemented by ferroelectric polarization switching dynamics of Al-doped HfO 2 ferroelectric gate insulators.
9 January 2020 in IEEE Transactions on Electron Devices
Nonvolatile memory characteristics of the ferroelectric field-effect transistors (FeFETs) were investigated by introducing the metal–ferroelectric–metal–insulator–semiconductor (MFMIS) gate-stacks, employing Al-doped HfO 2 (Al:HfO 2 ) ferroelectric thin films. The obtained memory window (MW) of the MFMIS FETs increased from 1.0 to 2.8 V by increasing the areal ratios of the metal–insulator–semiconductor (MIS) to the metal–ferroelectric–metal (MFM) (S I /S F ) from 8 to 32. The device with an S I /S F ratio of 16 exhibited a 3-order-of-magnitude on/off memory margin even with a program pulse duration of 500 ns. The long-term data retention was also verified by improving the tolerance against the depolarization field by introducing the MFMIS gate-stacks, which can use fully saturated polarization. The temperature-dependent memory performance and operational reliabilities of the MFMIS-FETs were also investigated at high temperatures to exploit fully the thermal stability of the Al:HfO 2 . The obtained MWs were not markedly degraded for a retention time of 10 4 s from room temperature (RT) to 80 °C.
Amorphous indium gallium zinc oxide thin-film transistors (TFTs) were fabricated and characterized on flexible poly(ethylene naphthalate) (PEN) substrates. A hybrid inorganic/organic double-layered barrier layer structure was proposed for enhancing the permeability and the surface roughness of the PEN substrates, which was composed of a 3 μm-thick spin-coated organic layer and a 50 nm-thick atomic-layer-deposited Al2O3 inorganic layer. The saturation mobility, subthreshold swing, and on/off ratio of the TFTs on the PEN substrates with the proposed hybrid barrier structure were found to be approximately 15.5 cm2 V−1 s−1, 0.2 V dec−1, and 2.2 × 108, respectively. These good TFT performances were not degraded even under the mechanical bending situation at a curvature radius of 3.3 mm and after the repetitive bending cycles. Furthermore, the variations in turn-on voltage of the TFT were evaluated to be approximately as small as −0.1 and +1.6 V under the negative and positive-bias stress tests, respectively.
Ferroelectric Hf0.5Zr0.5O2 (HZO) thin film capacitors with Pt/HZO/TiN structures were characterized to investigate the effects of oxygen partial pressure (PO2) and film thickness on the ferroelectric properties and switching dynamics of sputter-deposited HZO thin films. The PO2 during deposition and the film thickness varied from 0% to 1.5% and from 20 to 30 nm, respectively. The ferroelectric remnant polarization (2Pr) was 24.8 μC/cm2 for the 20-nm-thick HZO thin film deposited at a PO2 of 0% and decreased with increasing PO2 and film thickness due to variation in the amount of ferroelectric orthorhombic phase. The 2Pr of the 30-nm-thick HZO film deposited at a PO2 of 1% was 9.60 μC/cm2. The switching times and related parameters of the HZO films were estimated and analyzed by Kolmogorov–Avrami–Ishibashi and nucleation-limited switching (NLS) models. The NLS model provided better fitting results over the full range of polarization switching. The switching times could be modulated with variations in PO2 and film thickness from 0.46 to 1.58 μs. The activation field for polarization reversal increased with increasing PO2, and the degree of PO2 dependence was higher for a thinner film.