Electroless composite coatings were deposited on API X60 grade pipeline steel, and the effect of nickel sulfate, sodium hypophosphite, copper sulfate, and TiO 2 nanoparticle concentration on deposition rate, microhardness, and surface roughness was investigated using a Taguchi L27 experimental design coupled with grey relational analysis (GRA). Analysis of Variance (ANOVA) was used to determine the statistical significance of the process parameters. The optimized coating was subjected to post-deposition annealing at 200°C, 400°C, and 600 °C. Microhardness measurements, surface roughness analysis, field-emission scanning electron microscopy coupled with energy-dispersive spectroscopy, and x-ray diffraction were utilized to evaluate the coating characteristics. Sodium hypophosphite (P) and nickel sulfate (Ni) are identified as the dominant factors affecting microhardness (49.31% (P) and 38.78% (Ni)) and deposition rate (28.95% and 61.11%). In comparison, surface roughness is influenced by sodium hypophosphite (35.10%) and copper sulfate (Cu) (27.57%), as observed in the S/N ratio and ANOVA analysis. GRA optimum bath composition is 20 g l −1 nickel sulfate, 14 g l −1 sodium hypophosphite, 0.3 g l −1 copper sulfate, and 1 g l −1 TiO 2 . An experiment conducted under GRA-optimized conditions yielded a microhardness of 599 HV 0.05 , a surface roughness of 0.320 µ m, and a deposition rate of 13.08 mg.cm −2 .h −1 . Microstructural and phase analyses revealed a nodular, amorphous as-deposited coatings, while annealing promoted crystallization through the precipitation of Ni 3 P phase. The maximum hardness was obtained after heat treatment at 400 °C, whereas further increasing the annealing temperature to 600 °C resulted in a decrease in hardness and an increase in surface roughness, which was associated with microstructural changes and increased surface oxidation.