Yongchun Guo

Yongchun Guo

Auto-generated profile, based on publicly available information

Yongchun Guo

School of Defence Science and Technology, Xi? an Technological University, Xi' an, Shaanxi, China

Research Focus & Metrics

Academic Career Length

10Years (2017-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
18 July 2018 in Materials
Verified
Journal Article
Open access
PDF file
LTLusha Tian
Lusha Tian
YGYongchun Guo
Yongchun Guo
JLJianping Li
Jianping Li
FXFeng Xia
Feng Xia
MLMinxian Liang
Minxian Liang
YBYaping Bai
Yaping Bai
The effects of cooling rate 0.15, 1.5, 15, 150, and 1.5 × 105 °C/s on the microstructures and mechanical properties of Al-13Si-4Cu-1Mg-2Ni cast piston alloy were investigated. The results show that with an increase of solidification cooling rate, the secondary dendrite arm spacing (SDAS) of this model alloy can be calculated using the formula D = 47.126v − 1/3. The phases formed during the solidification with lower cooling rates primarily consist of eutectic silicon, M-Mg2Si phase, γ-Al7Cu4Ni phase, δ-Al3CuNi phase, ε-Al3Ni phase, and Q-Al5Cu2Mg8Si6 phase. With the increase in the solidification cooling rate from 0.15 to 15 °C/s, the hardness increased from 80.9 to 125.7 HB, the room temperature tensile strength enhanced from 189.3 to 282.5 MPa, and the elongation at break increased from 1.6% to 2.8%. The ε -Al3Ni phase disappears in the alloy and the Q phase emerges. The δ phase and the γ phase change from large-sized meshes and clusters to smaller meshes and Chinese script patterns. Further increase in the cooling rate leads to the micro hardness increasing gradually from 131.2 to 195.6 HV and the alloy solidifying into a uniform structure and forming nanocrystals.

1 May 2023 in Journal of Materials Engineering and Performance
Verified
Journal Article
Closed access
PDF file
JCJihui Chen
Jihui Chen
qiaoqin guoqiaoqin guo
qiaoqin guo
ZYZhong Yang
Zhong Yang
JLJianping LI
Jianping LI
YGYongchun Guo
Yongchun Guo
DXDapeng Xu
Dapeng Xu

1 September 2018 in Applied Sciences
Verified
Journal Article
Open access
PDF file
LTLusha Tian
Lusha Tian
YGYongchun Guo
Yongchun Guo
JLJianping Li
Jianping Li
FXFeng Xia
Feng Xia
MLMinxian Liang
Minxian Liang
JWJianli Wang
Jianli Wang
In the present paper, the microstructures of three kinds of in-situ reinforcements Al-Ti-C, Al-Ti-B, and Al-Ti-B-C-Ce were deeply investigated using a combination of scanning electron microscopy, X-ray diffraction spectroscopy, and transmission electron microscopy. The effect of in-situ reinforcements on the room temperature and elevated temperature (350 °C) tensile strengths of Al-13Si-4Cu-1Mg-2Ni alloy were analyzed. It is found that doping with trace amounts of B and Ce, the size of the Al3Ti phase in the in-situ reinforced alloy changed from 80 µm (un-reinforced) to about 10 µm, with the simultaneous formation of the AlTiCe phase. The Al-Ti-B-C-Ce reinforcement which is rapid solidified, was more effective and superior to enhance the tensile strengths of the Al-13Si-4Cu-1Mg-2Ni alloy, both at room and high temperatures than those of addition other reinforcements. The room temperature (RT) strength increased by 19.0%, and the 350 °C-strength increased by 18.4%.

19 September 2020 in Advanced Engineering Materials
Verified
Journal Article
Closed access
PDF file
YGYongchun Guo
Yongchun Guo
XGXusen Gao
Xusen Gao
FXFeng Xia
Feng Xia
ZMZhijun Ma
Zhijun Ma
WYWei Yang
Wei Yang
JLJianping Li
Jianping Li

7 August 2020 in Scanning
Verified
Journal Article
Open access
PDF file
YBYaping Bai
Yaping Bai
JLJianping Li
Jianping Li
JLJiajia Luo
Jiajia Luo
YGYongchun Guo
Yongchun Guo
The effect of diamond surface pretreatment and content on the microstructure and mechanical properties of NiAl/Fe–x diamond (x=0,5,10,15,and 20 wt.%) alloys was investigated after mechanical alloying with subsequent hot-pressing sintering. The results showed that after the surface pretreatment, a complete transition layer containing W existed on the outer surface of the diamond grains, which improved the interfacial bonding strength of the diamond grains and NiAl/Fe matrix to an excellent level. As the diamond content increased, the compressive strength of the NiAl/Fe-based alloys declined, but the alloy with 10 wt.% diamond had a higher value than that of the other NiAl/Fe-based alloys. Short cracks and transgranular fracture were observed in the fracture surface of all materials. For the material with 20 wt.% diamond, intergranular fracture was obvious, and many diamond particles appeared along the fracture direction, which caused the compressive strength to be the lowest of the samples considered in this study. After the addition of diamond, the oxidation resistance of NiAl/Fe-based alloys decreased due to a loose oxidation layer and diamond graphitization. The thermal conductivity of the alloy first increased and then decreased with increasing diamond content. A NiAl/Fe-based alloy with 15 wt.% diamond demonstrated the maximum thermal conductivity of 53.2 W/(m·k) at 600°C among the samples in this study.

30 March 2017 in Surface Review and Letters
Verified
Journal Article
Closed access
PDF file
YBYaping Bai
Yaping Bai
JXJiandong Xing
Jiandong Xing
YGYongchun Guo
Yongchun Guo
JLJianping Li
Jianping Li
QHQian Huang
Qian Huang
YGYimin Gao
Yimin Gao