Cellulose nanocrystals (CNC) were mixed with either cellulose nanofibril (CNF) or carboxymethylcellulose (CMC) in variable proportions (0/100, 20/80, 40/60, 50/50, 60/40, 80/20 and 100/0) to obtain cast films with acceptable barrier and mechanical properties as replacements for food packaging plastics. Both CNF and CMC improved tensile strength, elongation, UV opacity, air resistance, hydrophobicity (WCA-water contact angle), water vapor transmission rate (WVTR) and oxygen impermeability in pure CNC. WVTR and oxygen permeability were strongly dependent on relative humidity (RH). Interestingly, the greatest effect on WVTR was observed at RH = 90% in films containing CMC in proportions above 60%. CMC- and CNF-containing films had oxygen impermeability up to an RH level of 80% and 60%, respectively. The previous effects were confirmed by food packaging simulation tests, where CMC-containing films proved the best performers. The composite films studied were biodegradable-which constitutes a major environmental related advantage-to an extent proportional to their content in CMC or CNF.
Preparation of nanocrystalline cellulose (NCC) by 62 and 65 % wt. sulfuric acid hydrolysis of cellulase-pretreated fibers was optimized to obtain the highest yield by applying two statistical plans. At optimal conditions (10 U/g odp cellulase, 25 min hydrolysis, 47 °C, 62 wt.% H2SO4), high yields (≥80 %) were obtained, including an increase of ~9 points due to the enzyme. Optimal conditions produced nanosized particles of around ~200 nm with reduced surface charge and sulfur content. The optimization allowed reduction of hydrolysis time by 44 % and increase of yield by more than 10 points compared with results in previous work. The effects of cellulase pretreatment were noticeable even under aggressive hydrolysis conditions, emphasizing its possibilities. Zeta potential and polydispersity index indicated that all studied conditions led to good-quality final products, with values around −50 mV and 0.2, respectively. Transmission electron microscopy (TEM) analysis confirmed the presence of NCC. Fourier-transform infrared (FTIR) spectroscopic analysis provided evidence that cellulase treatment increased the crystallinity of both cellulose fibers and NCC, as well as fiber accessibility, supporting the other analyses of NCC.
Antioxidant activity of xylooligosaccharides (XOS) released from beechwood and birchwood glucuronoxylans by two different xylanases, one from family GH10 (Xyn10A) and another from family GH30 (Xyn30D) was examined. The ABTS (2, 2'-Azino-bis(3-ethylbenzothiazoline-6-sulfonic acid)) method was used, since it resulted more accurate for the antioxidant activity determination of XOS. Thin layer chromatography and MALDI-TOF MS analysis showed that Xyn10A produced a mixture of neutral and acidic XOS whereas the XOS produced by Xyn30D were all acidic, containing a methylglucuronic acid (MeGlcA) ramification. These acidic XOS, MeGlcA substituted, showed a strongly higher antioxidant activity than the XOS produced by Xyn10A (80% vs. 10% respectively, at 200 μg mL-1). Moreover, the antioxidant activity increased with the degree of polymerization of XOS, and depended on the xylan substrate used. The antioxidant capacity of eucalyptus autohydrolysates after xylanase treatment was also analysed, showing a decrease of their antioxidant activity simultaneous with the decrease in XOS length.