Hui-Dong Qian

Hui-Dong Qian

Auto-generated profile, based on publicly available information

Hui-Dong Qian

Institute of Condensed Matter and Material Physics, School of Physics, Peking University 1 , Beijing 100871

Research Focus & Metrics

Academic Career Length

10Years (2017-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 November 2018 in Journal of Alloys and Compounds
Verified
Journal Article
Closed access
YYYang Yang
Yang Yang
JKJong-Woo Kim
Jong-Woo Kim
PSPing-Zhan Si
Ping-Zhan Si
HQHui-Dong Qian
Hui-Dong Qian
YSYongho Shin
Yongho Shin
CCChul-Jin Choi
Chul-Jin Choi

1 April 2019 in Journal of Magnetism and Magnetic Materials
Verified
Journal Article
Closed access
PSP.Z. Si
P.Z. Si
YYY. Yang
Y. Yang
LYL.L. Yao
L.L. Yao
HQH.D. Qian
H.D. Qian
HGH.L. Ge
H.L. Ge
CCC.J. Choi
C.J. Choi

31 August 2017 in Materials
Verified
Journal Article
Open access
PDF file
PSPing-Zhan Si
Ping-Zhan Si
HQHui-Dong Qian
Hui-Dong Qian
CCChul-Jin Choi
Chul-Jin Choi
Jihoon ParkJihoon Park
Jihoon Park
SHSangho Han
Sangho Han
KSKiran P. Shinde
Kiran P. Shinde
The phase transformation in two modes, including both displacive and massive growth of τ-phase from ε-MnAl(C), was observed by in situ transmission electron microscopy. The exact temperature range for different phase transformation modes was determined by magnetic measurements. The displacive growth of ε→τ in Mn54Al46 (or Mn54Al46C2.44) occurs at temperatures below 650 K (or 766 K), above which both modes coexist. One-third or less of the ε-phase can be transformed into τ-phase via displacive mode while the remaining two-thirds or more via massive mode. In bulk τ-phase, most τ-nanocrystals formed via displacive mode are distributed in the matrix of large τ-grains that formed via massive mode. The typical massive growth rate of the τ-phase is 8–60 nm/s, while the displacive growth rate is low. A more complete understanding of the ε→τ phase transformations in the MnAl-based magnets was provided in this work, based on which the annealing process for ε→τ was optimized and thus high purity τ-phase with high saturation magnetization was obtained.

1 April 2018 in Journal of Magnetism and Magnetic Materials
Verified
Journal Article
Closed access
PSPing-Zhan Si
Ping-Zhan Si
HQHui-Dong Qian
Hui-Dong Qian
CCChul-Jin Choi
Chul-Jin Choi
JPJihoon Park
Jihoon Park
HGHong-Liang Ge
Hong-Liang Ge

19 November 2018 in Journal of Electronic Materials
Verified
Journal Article
Closed access
PDF file
PSPing-Zhan Si
Ping-Zhan Si
HQHuidong Qian
Huidong Qian
XWXinyou Wang
Xinyou Wang
YYYang Yang
Yang Yang
JPJihoon Park
Jihoon Park
CCChul-Jin Choi
Chul-Jin Choi

7 May 2018 in Applied Physics Letters
Verified
Journal Article
Open access
PDF file
PSPing-Zhan Si
Ping-Zhan Si
HQHui-Dong Qian
Hui-Dong Qian
HGHong-Liang Ge
Hong-Liang Ge
JPJihoon Park
Jihoon Park
CCChul-Jin Choi
Chul-Jin Choi
Little is known about the physical properties of Mn4C for which is unstable and difficult to prepare. We herein report on the unusual thermomagnetic properties of high purity Mn4C powders obtained by plasma melting and magnetic separation processes. The saturation magnetization of Mn4C increases linearly with increasing temperature in the range of 50 K–590 K and remains stable at temperatures below 50 K. The anomalous magnetization increases of Mn4C with increasing temperature can be considered in terms of the Néel's P-type ferrimagnetism. At temperatures above 590 K, the Mn4C decomposes into Mn23C6 and Mn, which would be partially oxidized into manganosite when exposed to air. The remanent magnetization of Mn4C varies little with temperature. The Curie temperature of Mn4C is around ∼870 K. The positive temperature coefficient (∼0.0072 Am2 kg−1 K−1) of magnetization in Mn4C makes it potentially important in controlling the thermodynamics of magnetization in magnetic materials.