23 June 2016 in Journal of Materials Chemistry C
Indium oxide thin films are deposited via plasma-enhanced atomic layer deposition (PEALD) to exploit their potential as a semiconductor in high mobility thin-film transistors (TFTs), which are suitable for fast driving applications such as high resolution displays. The films are successfully grown by the reaction between an Et2InN(SiMe3)2 liquid precursor and oxygen plasma at temperatures ranging from 100 °C to 250 °C giving a saturated growth rate value of ∼1.45 Å per cycle at the ALD window with precisely controlled thickness and uniformity. The plasma reaction enhances the film growth rate and changes the electrical properties of the films. Depending on the substrate temperatures, each film has a different chemical composition, thereby showing different electrical characteristics. Indium oxide films grown by PEALD show a lower carrier density of ∼4 × 1019 cm−3 than those prepared by thermal ALD due to the reactive oxygen plasma source in the former. Offering the precise control of thickness and high quality of indium oxide grown by PEALD, and with a proper post thermal-annealing and passivation process, the possibility of exploiting the potential of semiconductor characteristics of indium oxide is verified from bottom-gate coplanar structured TFTs, which exhibit a high mobility as high as 39.2 cm2 V−1 s−1, a turn-on voltage value of −1.18 V, and a sub-threshold voltage of 0.27 V dec−1 in a linear region. On the basis of this outstanding performance, the PEALD-InOx TFTs developed in this study would be suitable for diverse microelectronic devices.
26 February 2020 in ACS Applied Materials & Interfaces
15 August 2021 in ACS Applied Materials & Interfaces
16 February 2020 in Journal of Materials Chemistry C
Flexible and wearable pressure sensors, which can detect various pressures generated by the human body and convert them into electrical signals, are of great interest because they have a wide variety of applications for an interface between humans and external devices. Elastomeric dielectric materials for commercial piezocapacitive pressure sensors need to be manufactured quickly and easily via cost-effective methods. Herein, we report a piezocapacitive pressure sensor based on a three-dimensional macroporous dielectric layer fabricated by a rapid and facile baking-inspired foaming process. The pressure sensor showed high sensitivities of 0.16 ± 0.03 kPa−1 (at <1 kPa) and 0.14 ± 0.02 kPa−1 (at 1–10 kPa) and a low detection limit of 9.8 Pa. Furthermore, 10 000 repetitive compressing and releasing cycles confirmed its reliability. We established that the pressure sensor could move virtual fingers by detecting finger gripping pressure in real time. The respiration rate was also detected by the pressure sensor. A large-scale pressure sensor array was constructed to demonstrate a scaled-up fabrication process. The array accurately recognized spatially distributed pressures generated by objects.
21 December 2022 in Journal of Materials Chemistry C
Rectifying diodes have emerged as one of the promising components for advanced functional devices, including resistive random access memory and backplanes of active-matrix systems. Among various types of diodes, oxide thin film diodes have been extensively studied for their outstanding stability and rectifying characteristics. In this study, we developed a metal–oxide semiconductor–insulator–metal (MSIM) diode by atomic layer deposition-assisted interface engineering and obtained a high on–off ratio of ∼108, low off-current density of 10−9 A cm−2 and good reliability. For the first time, the operation mechanism of the MSIM diode was also scrutinized with chemical analyses. X-Ray photoelectron spectroscopy and density functional theory results indicate that trimethylaluminum induced oxygen vacancies at the interface between InOx and Al2O3 through a reduction reaction during Al2O3 deposition. The induced oxygen vacancies promote the formation of abundant tail states near the interface, and the tail states contribute to the injection of electrons from the cathode into Al2O3. From chemical and electrical analyses, suitable conduction mechanism and energy band diagram of the MSIM diode were proposed in detail. Consequently, the MSIM diode has been successfully demonstrated on a flexible polyimide substrate without degradation of rectifying characteristics, providing the potential of the MSIM diode as an advanced electronic device.
1 September 2016 in ECS Meeting Abstracts
With the development of the virtual reality and augmented reality displays, ultra-high resolution displays become one of the big concerns. People would not be bothered by display pixels when taking closer look at display with the resolution higher than 2000 ppi. The most important factor in the ultra-high resolution display is the pixel area and the smallest TFT size would be the first criteria in the TFT point of view. Although back channel etch (BCE) TFT and self-aligned (SA) TFT have been used for driving high resolution LCD and OLED, respectively, typical planar structured TFT would not permit display with ultra-high resolution. The vertical TFT with the smallest pixel pitch value among the TFT structures is suitable candidate. Furthermore, channel length of the vertical TFT can be precisely controlled by the thin film thickness of spacer. This results in high and uniform on-current of TFT. Meanwhile, vertical TFT can also provide channel length longer than the sub-pixel length. When we have to apply high gate voltage depending on the display mode, TFT with longer channel length within smaller sub-pixel size would be necessary. One of the advantages of oxide TFTs lies in the freedom of selection of architecture, materials, and process depending on the device application. Considering the main issue in the vertical TFT, the step coverage of active layer, oxide TFT seems to be the best selection. Oxide semiconductor and gate insulator used for the oxide TFT can be deposited by means of plasma enhanced atomic layer deposition (PEALD), which provides excellent step coverage of films. One of the issues in vertical oxide TFT is the relatively high off-current depending on the mobility of TFT due to the short channel length. Here, we compare the performance of vertical oxide TFTs with the variation of semiconductor’s carrier density. By virtue of the easiness for the modifying carrier concentration of InOx based semiconductor, we could adjust the mobility of vertical TFT with low off-current. Vertical TFT with InOx shows 1.26 mA at Vg = 5 V and Vds = 2.1 V, S.S of 0.14 V/dec., on/off ratio of 107, and Von of -1.8V. Meanwhile at the same driving condition, IGZO shows on-current of 0.23 mA, S.S of 0.12 V/dec., on/off ratio of 108 and Von of -0.2V. We will discuss the best selection for the channel layer of vertical TFT depending on the display mode and show the optimized TFT performance depending on the carrier concentration of semiconductors.