We studied the effect of systematically-controlled size (22–83 nm) and density (0.1–13 × 1021 m−3) of strong pinning random BaMO3 (M=Zr, Nb, Sn) nanoparticles (NPs) by engineering of their inclusion in (Y0.77Gd0.23)Ba2Cu3Oy ((Y,Gd)BCO) coated conductors. The critical current density (Jc) gradually increases from that of pure (Y,Gd)BCO to that of 3 wt% BZO with increasing density of NPs for H ‖ c and H ‖ 45°. Moreover, at low/intermediate fields the films with higher densities of isotropic pinning centers show nearly isotropic angular dependence at both 77 and 65 K, indicating that a high density of spherical nanoparticles effectively pins vortices over a broad angular range. We find that the enhancement of Jc depends mainly on the density of the NPs and not on their size. The vortex melting transition (characterized by the critical exponent (s) of the resistive transition) changes, particularly at H ‖ 45° in films with higher densities of NPs. This change is reflected in a decrease of s to a value very close to that observed for H ‖ c, similar to that of a Bose-glass. Thus, the density and morphology of the pinning centers are important factors determining not only Jc but also the character of the solid–liquid transition.
Because of pressing global environmental challenges, focus has been placed on materials for efficient energy use, and this has triggered the search for nanostructural modification methods to improve performance. Achieving a high density of tunable-sized second-phase nanoparticles while ensuring the matrix remains intact is a long-sought goal. In this paper, we present an effective, scalable method to achieve this goal using metal organic deposition in a perovskite system REBa2Cu3O7 (rare earth (RE)) that enhances the superconducting properties to surpass that of previous achievements. We present two industrially compatible routes to tune the nanoparticle size by controlling diffusion during the nanoparticle formation stage by selecting the second-phase material and modulating the precursor composition spatially. Combining these routes leads to an extremely high density (8 × 1022 m−3) of small nanoparticles (7 nm) that increase critical currents and reduce detrimental effects of thermal fluctuations at all magnetic field strengths and temperatures. This method can be directly applied to other perovskite materials where nanoparticle addition is beneficial.
We show a simple and effective way to improve the vortex irreversibility line up to very high magnetic fields (60T) by increasing the density of second phase BaZrO3 nanoparticles. (Y0.77,Gd0.23)Ba2Cu3Oy films were grown on metal substrates with different concentration of BaZrO3 nanoparticles by the metal organic deposition method. We find that upon increase of the BaZrO3 concentration, the nanoparticle size remains constant but the twin-boundary density increases. Up to the highest nanoparticle concentration (n ~ 1.3 × 1022/m3), the irreversibility field (Hirr) continues to increase with no sign of saturation up to 60 T, although the vortices vastly outnumber pinning centers. We find extremely high Hirr, namely Hirr = 30 T (H||45°) and 24 T (H||c) at 65 K and 58 T (H||45°) and 45 T (H||c) at 50K. The difference in pinning landscape shifts the vortex solid-liquid transition upwards, increasing the vortex region useful for power applications, while keeping the upper critical field, critical temperature and electronic mass anisotropy unchanged.
1 February 1992 in Journal of Magnetism and Magnetic Materials
(Y 0.77 Gd 0.23 )Ba 2 Cu 3 O y [(Y,Gd)BCO] films were grown on CeO 2 buffered R -plane sapphire ( R -Al 2 O 3 ) substrates using trifluoroacetate metal organic deposition (TFA-MOD). Annealing of the CeO 2 buffered R -Al 2 O 3 substrates was performed to control the crystallinity and surface morphology of the CeO 2 buffer layer. The annealing treatment led to a significant improvement in the crystallinity and surface morphology of the CeO 2 buffer layer. A (Y,Gd)BCO film grown on the CeO 2 buffer layer with high crystallinity and an atomically flat surface exhibited high self-field (at 77 K) and in-field (at 20 K, 9 T, μ 0H ∥ c ) critical current densities ( Jc ). Annealing of the CeO 2 buffer layer thus enabled enhancement of not only the self-field Jc for the (Y,Gd)BCO film but also the in-field Jc .