1 May 2021 in Materials Science and Engineering: A
4 November 2020 in Advanced Engineering Materials
Fe–TiC metal matrix composite powder is manufactured applying vacuum inert gas atomization technique. The TiC reinforcement phase forms in situ within spraying of the Fe‐based molten metal preliminary alloyed with 1 wt% [C] and 4 wt% [Ti]. Alloying strategy, homogenization time, and spraying temperature are varied for three conducted atomization experiments in this study. Medium particle size (d50) lies in a range of 41–55 μm for obtained spherical powders. Scanning electron microscopy (SEM) analysis and Energy‐dispersive X‐ray spectroscopy (EDX) mapping of powder cross‐section samples reveal well‐dispersed submicron TiC precipitates of two different morphologies—primary‐blocky and eutectic‐plate‐shape carbides. The amount of precipitates and their morphology depend on the particle size. Namely, coarser powder particles tend to have more primary carbides that are presumably formed already in liquid droplets. Meanwhile, TiC precipitation in finer particles up to ≈25 μm is completely suppressed due to an extremely high cooling rate. Difficulties of the Fe–Ti–C melt atomization (e.g., formation of a semiliquid slag layer, loss of TiC forming elements, the presence of large precipitates in a powder) are discussed considering the thermodynamic analysis of this system and Fe–TiC remelting experiments conducted on a hot stage microscope.
20 September 2023 in Advanced Engineering Materials
Fe–xTiC in situ metal matrix composites (MMCs) are fabricated utilizing a cold crucible inductive melting (CCIM) technique with varying TiC amounts (2, 3.5, and 5 wt%). Steel blocks and pure Ti plates are remelted in a water‐cooled copper crucible. The subsequent solidification of [Ti]‐ and [C]‐rich melt yields TiC reinforcement particles in an ingot. The holding time varies between 5 and 30 min, whereas the holding temperature alters depending on the amount of TiC, ranging from 1380 to 1620 °C for Fe‐5TiC and Fe‐2TiC, respectively. Alloying efficiency for TiC‐forming elements is estimated for all fabricated Fe–xTiC ingots by comparing [Ti] and [C] target values with measured ones. The lower TiC amounts and shorter holding times result in decreased [Ti] and [C] losses. SEM analysis of three cross‐section samples representing different TiC amounts reveals two distinct morphologies of TiC in situ reinforcements: primary blocky/cubic and eutectic plate‐like precipitates. The blocky precipitates appear slightly finer with a decrease in TiC amount (4.4 ± 1.2 μm for Fe‐5TiC and 3.8 ± 0.7 μm for Fe‐2TiC), whereas the length of plate‐like precipitates noticeably decreases in the samples with lower TiC amounts (11.0 ± 7.0 μm for Fe‐5TiC and 6.8 ± 3.6 μm for Fe‐2TiC).
11 August 2022 in Ceramics International
28 May 2024 in Steel Research International
The remelting of Fe‐xTiC metal matrix composites (MMCs) is studied using the sessile drop method. This is to determine the conditions needed for the complete dissolution of TiC precipitates in the Fe‐based melt. Samples with different amounts of TiC (2, 3.5, and 5 wt%) are analyzed in a hot‐stage microscope (HSM), capturing the softening and melting temperatures. A Cr‐alloyed steel is selected as a matrix. Consequently, the presence of TiC elevates the melting initiation temperature above the melting point of pure iron (e.g., 1659 ± 10 °C for Fe‐5TiC). Furthermore, samples with higher TiC amounts exhibit higher melting initiation temperatures. This trend is confirmed by differential scanning calorimetry measurements, conducted on the representative Fe‐xTiC samples. Microstructural examinations of the solidified (HSM) samples identify two distinct TiC precipitate morphologies: primary blocky/cubic and secondary eutectic plate like. For instance, the Fe‐5TiC sample contains numerous blocky/cubic precipitates (7.5 ± 3.1 μm) clustered at the upper cross‐ section, while secondary plate‐like precipitates (20.4 ± 11.8 μm) are uniformly distributed in eutectic assemblies with the matrix. This study provides meaningful insights for optimizing the production of as‐cast and as‐atomized Fe‐TiC MMCs, particularly in selecting reinforcement levels and homogenization temperatures for complete TiC dissolution.