Background. When silver diamine fluoride (SDF) is used in conjunction with conservative caries removal in deep carious lesions, the distribution depth of silver is critical for safety and effectiveness. Objective. The purpose of this study is to determine the effect of selected caries removal on silver penetration when 38% SDF is applied to deep carious lesions in permanent teeth. Methods. Extracted permanent teeth with caries extending to the inner third of the dentin were used (N = 18). The periphery of the carious lesion was completely removed to the dentinoenamel junction (DEJ). In group A (n = 9), no further removal of carious tissue was performed, leaving necrotic dentin inner to the DEJ, whereas in group B (n = 9) superficial necrotic dentin was completely removed until leathery, slightly moist, reasonably soft dentin remained. SDF was applied for 3 minutes in both groups. Microcomputer tomography (micro-CT) and field emission scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy (FESEM-EDS) were used to measure mineral density and silver distribution. The silver penetration depth/lesion depth (PD/LD) ratio was calculated for each sample. The Mann–Whitney U test was used to compare differences between the two groups. Results. The micro-CT analysis showed that the PD/LD ratios of group B (1.07–2.29) were marginally greater than those of group A (1.00–1.31). However, a statistically significant difference was not observed (value = 0.5078). When stratified by remaining dentin thickness (RDT), the PD/LD ratios of group B were still greater than those of group A only when RDT was >500 µm. The FESEM-EDS analysis indicated that silver particles precipitated throughout the entire thickness of the carious lesions. Conclusion. Applying SDF on a deep carious lesion and leaving the necrotic dentin pulpally did not affect silver penetration. However, the extent to which silver penetrates the remaining dentin beneath the lesions is dependent on the amount and characteristics of that dentin.
Resin-based composites tend to have a limited service lifetime, primarily due to the hydrolytic and enzymatic degradation of the relatively susceptible methacrylate-based components used in dental resin adhesives. To address these limitations, a series of methacrylamide- and acrylamide-based self-etching monomers were synthesized. These four monomers incorporated a long alkyl chain, a (meth)acrylamide polymerizable group, and a phosphonic acid adhesive moiety, with the aim of enhancing hydrolytic stability. All synthesized (meth)acrylamide monomers exhibited comparable or lower cytotoxicity and greater hydrolytic stability under acidic conditions than the conventional self-etching methacrylate monomer, 10-MDP. Changes in the 13C and 31P NMR chemical shifts suggested ionic interactions between the dissociated phosphonic acid groups and calcium ions in hydroxyapatite. Among the tested formulations, the resin adhesive incorporating 10-AADP exhibited the lowest water solubility, which was attributed to the greater hydrolytic stability of the amide bonds. It also showed lower water sorption than the 10-MDP-containing adhesive, potentially due to stronger hydrogen bonding within the polymer network, resulting in the highest flexural strength and flexural modulus. The higher pKa values of 10-AADP compared with 10-MDP indicate milder acidity, which may provide a more self-limiting etching effect and potentially improve preservation of the dentin–resin interface. Overall, the hydrolytic stability, strong adhesion to tooth mineral, high degree of conversion and low cytotoxicity of 10-AADP demonstrate its potential as a durable alternative self-etching monomer for use in dentin primers.