27 March 2023 in Journal of Traffic and Transportation Engineering (English Edition)
1 June 2019 in Journal of Materials in Civil Engineering
Asphalt binders and concretes modified with polyacrylonitrile (PAN) fiber, styrene butadiene styrene (SBS), and the combination of PAN-SBS were prepared and studied. Both frequency and temperature sweep tests for the binder dynamic shear modulus G*, rutting, and fatigue parameters were carried out. Multiple stress creep recovery (MSCR) test was also conducted on the various modified asphalt binders. The complex modulus E* and flow number (FN) of asphalt concretes (AC) from the modified binders were also examined using asphalt mixture performance tester (AMPT) test. The PAN fiber asphalt binder showed better response in terms of dynamic modulus, fatigue and rutting parameter, nonrecoverable creep compliance and percent strain recovery at 1% fiber content. The hybrid binder ( ) demonstrated overall shear modulus almost twice that exhibited by 2%SBS binder. The hybrid asphalt binder showed the greatest potential for rut resistance, over most of the frequency range, relative to all other binders. It was clear that the combined form of the polymer and the fiber modification has greater rutting resistance potential than the single modification approach generally practiced. The hybrid asphalt binder also showed better fatigue parameter than all the binders within pavement design load frequency range. Results from the AC mix tests verified most of the trends observed from the asphalt binder tests.
1 November 2018 in International Journal of Pavement Research and Technology
5 June 2018 in Arabian Journal for Science and Engineering
6 June 2020 in International Journal of Pavement Engineering
Multiple Stress Creep and Recovery (MSCR) test was conducted on four different types of polymer-modified asphalt (PMA) with three different performance grade (PG) levels, at two stress levels (0.1 and 3.2 kPa) and four temperatures (58 degrees C, 64 degrees C, 70 degrees C and 76 degrees C). Strain recovery rates, absolute per cent recovery and creep compliance recovery rate of the PMAs at near instantaneous (NI) and near steady-state (NSS) regions were estimated and analysed. Higher levels of applied stress and temperature have induced a correspondingly higher rate of strain recovery both at NI (RRNI) and NSS, due to additional rebound energy accompanying more sustained deformation. Similar but mild strain recovery rate trend was observed with increasing PG. The strain recovery rate is inversely proportional to the per cent strain recovered, for a given temperature and applied stress, both at NI and at NSS region. An absolute per cent recovery at NI (%R-NI) and NSS (%R-NSS) was estimated in terms of the strain recovery rates. The %R-NI is relatively constant for all rest periods, and can be obtained within the first 2 seconds of the creep-recovery cycle. Finally, even though the conventional MSCR parameters (i.e. J(nr) and R) showed statistically significant correlation with the AC rutting, some strain recovery rate base parameters (%R-NI and %R-NSS) demonstrate a statistically better correlation with the AC rutting.