Silver (Ag) substituted ZnO thin films were successfully deposited onto glass substrates by spray coating technique. Structure, morphology, and optical properties were evaluated by X-ray diffractometer (XRD), scanning electron microscopy (SEM), and UV-Vis spectrophotometer, respectively. XRD spectra had polycrystalline wurtzite structure; SEM images showed that thin films had different surface morphology at different Ag doping concentration. From transmittance spectra, thin films transparency decreased as well as band gap energy along with increase of Ag doping concentration. Methylene blue (MB) solution was used as a pollutant in the photodegradation studies. Under UV light irradiation, the optimal Ag doping is 25%, with 83% of the decolorizing efficiencies after 3 h irradiation time and apparent constant () about 9.69 × 10−3 min−1.
Zinc oxide (ZnO) and aluminum doped zinc oxide (ZnO:Al) thin films have been deposited onto a glass substrate by sol-gel spray coating method at atmospheric pressure. X-ray diffractometer (XRD), scanning electron microscopy (SEM), and UV-Vis spectrophotometer have been used to characterize the films. XRD spectra indicated that all prepared thin films presented the wurtzite hexagonal structure. SEM images exhibited rootlike morphology on the surface of thin films and the shortest root diameter was about 0.219 μm. The UV-Vis absorption spectra exhibited the absorption edges that were slightly shifted to the lower wavelength. From this result, the incorporation of aluminum into the ZnO involved a slight increase in the optical band-gap of films. The optical bands of films were 3.102 eV, 3.115 eV, 3.118 eV, 3.115 eV, 3.109 eV, and 3.109 eV for ZnO, ZnO:Al 2%, ZnO:Al 4%, ZnO:Al 6%, ZnO:Al 8%, and ZnO:Al 10%, respectively. Increase of Al doping concentration in ZnO films contributed to the increase of their optical band-gap which can be explained by the Burstein-Moss effect.
ZnO doped with 2~6 mol% Silver (Ag) photocatalyst thin films has been deposited on glass substrate by thermal spray coating with temperature deposition of 250°C. A gel of ZnO:Ag precursor has been synthesized by sol-gel route from aqueous/alcoholic solution of zinc acetate dehydrate and silver nitrate mixture at room temperature. The morphology of ZnO:Ag films were investigated scanning electron microscopy (SEM). 3D SEM images of ZnO:Ag thin films show the rough morphology with roughness mean square (rms) of 150 to 195 nm. The grain size of ZnO:Ag films were found in the range 76,5 to 304,8 nm. The photoactivity examination of ZnO:Ag photocatalyst films show the E. Coli bacteria degraded up to 99.99% under sunlight irradiation for 4 hours.
N-ZnO thin layer is widely used in application of wastewater photo catalyst. N-ZnO thin films have been successfully deposited on glass substrate using spray coating technique at 450 °C with varying concentrations of N from Urea source. XRD test results showed that the N-ZnO has a polycrystalline structure with diffraction field (100), (002), (101) and (110). The presence of nitrogen atoms in the lattice of ZnO causes a shift in diffraction angle between 0.08o - 0.18o. N-ZnO thin layer showed the occurrence of tensile strain. Surface morphology of N-ZnO is shaped like mine (like root). All samples have band gap energies lower than that of ZnO and the smallest is sample N6 with Eg = 3.249 eV. The presence of nitrogen atom increases surface roughness and decreases band gap energy.
Titanium dioxide (TiO2) is one of popular semiconductor materials that usually used for photocatalytic application. Recent studies show the improvement of TiO2 photocatalytic activity through nitrogen doping (N-doped TiO2). In this study, we focused on the synthesis and characterization of N-doped TiO2. Ultrasonic assisted synthesis or sonochemical method was used to prepare N-doped TiO2 polycrystalline powder under room temperature. X-ray diffractometer (XRD), and diffuse reflectance ultraviolet-visible spectrophotometer (DR-UV) were employed to evaluate physical properties of N-doped TiO2. XRD pattern exhibited that all samples have anatase crystalline phase and crystallite size decrease with increase of N dopant concentration. The absorbance spectra showed the slight shift toward higher wavelength (red shift) and from Kubelka-Munk function the band gaps were getting smaller with increase of N content. The increase of photocatalytic activity under solar radiation was achieved by N-doped TiO2 samples with highest efficiency about 81 % for 5% of N doping concentration.