2 February 2020 in Tribology - Materials, Surfaces & Interfaces
The present work focuses on investigating the wear and friction characteristics of the Atmospheric Plasma Sprayed Cr3C2-NiCr coatings deposited onto the surface of die steel material. The as-sprayed specimens were characterized. The coating porosity, bond strength and microhardness values were evaluated. Wear tests were performed on the high-temperature pin-on-disc tribometer at room temperatures, 400°C and 800°C under two loads as 25N and 50N in the laboratory. The wear mechanisms of all the worn-out samples were studied by scanning electron microscopy (SEM) technique. The specific wear rates and the coefficient of friction values were analyzed. The developed coating showed better wear resistance than its uncoated counterpart. The coefficient of friction values for coated specimens decreased at elevated temperatures. At room temperatures, the wear mode was observed to be adhesive and further at elevated temperatures of testing, the wear mode was observed to be the combination of oxidative, adhesive and abrasive.
1 January 2020 in Materials Today: Proceedings
26 February 2020 in Journal of Tribology
Wear and surface damage of tools (die materials) in hot metal forming industry is a critical problem observed and is producing an adverse effect on the process economy. The problem occurs when tool and workpiece interact at higher temperatures. However, the research related to the wear and friction of dies is still lacking. In the present investigation, the tribological (wear and friction) studies were conducted with an aim to explore the potential of Cr3C2-NiCr surface coating. The coating was developed onto the surface of hot forming tool steel materials by the HVOF spray technique. The mechanical and physical properties of the coatings were determined. Subsequently, wear and friction studies were conducted utilizing a high-temperature tribometer at two different loads and at three temperatures. Specific wear rates and the average coefficient of friction values were evaluated. Wear mechanisms were studied by scanning electron microscopy (SEM) technique. The wear mechanisms were observed to be adhesive in nature at room temperatures and the combination of abrasive/oxidative/adhesive in nature at higher temperatures for the Cr3C2-NiCr coated specimens.