20 November 2022 in Fine Chemical Technologies
Objectives. To obtain experimental data on the effect of activating additive type on the cold sintering process of (MnFeCoNiCu)3O4 high-entropy ceramic. The following substances were used as activating additives: ammonium acetate (CH3COONH4), acetic acid (CH3COOH), ammonium chloride (NH4Cl), potassium fluoride dihydrate (КF·2H2O), lithium fluoride (LiF), sodium fluoride (NaF), and sodium hydroxide (NaOH).Methods. Synthesis of the initial powder by low-temperature self-propagating method; investigation of the powder particles size distribution by laser diffraction method; analysis of the particle shape and compacted sample microstructure by scanning electron microscopy; investigation of the phase composition by X-ray phase analysis; high-entropy ceramic sample consolidation by cold sintering process. The density of the initial powder and the relative density of cold sintered samples were determined by the Archimedes method.Results. Samples with a relative density of over 0.70 were obtained using distilled water, CH3COONH4 and NaOH during cold sintering at 300 °C, with a holding time of 30 min and pressure 315 MPa.Conclusions. For the first time, the effect of the type of activating additive on the relative density of high-entropy ceramics (MnFeCoNiCu)3O4 samples obtained by cold sintering process has been experimentally demonstrated. The samples microstructures have pronounced differences: 20 wt % distilled water does not lead to grain growth, with only their compaction to 0.71 relative density observed; however, the addition of 0.1 wt % CH3COONH4 and NaOH increases the average grain size when reaching similar relative densities (0.70 and 0.71, respectively). X-ray diffraction analysis showed that the cold sintering process does not lead to a change in the phase composition of the initial (MnFeCoNiCu)3O4 powder, confirming the preservation of the high-entropy structure.
12 September 2024 in Fine Chemical Technologies
Objectives. To obtain porous corundum ceramics using an innovative cold sintering process starting from different phase modifications of aluminum oxohydroxide — boehmite γ-AlOOH and diaspore α-AlOOH; to study the phase and structural properties of the resulting materials; and to assess their permeability to water.Results. Cold sintering enables the formation of single-phase corundum ceramics with an open porosity of 47.9% directly from the initial boehmite powder with the addition of 5 wt % corundum in the presence of 20 wt % water at a temperature of 450°C, mechanical pressure of 220 MPa, and isothermal exposure for 30 min. Under the same conditions of cold sintering, a mixture of diaspore and boehmite was transformed into α-AlOOH ceramics. This then turned into corundum with an open porosity of 39% when calcined in air at 600°C for 1 h. The resulting materials had permeability for pure water above 5000 L/(m2∙h∙bar).Conclusions. Cold sintering is a promising approach to producing porous corundum ceramics which can be used in filtration systems. Compared to traditional ceramic technology, the new approach reduces energy, time, and labor costs in the material manufacturing. It also eliminates the need to use auxiliary substances (binders, pore-forming agents, etc.).
10 September 2026 in Fine Chemical Technologies
Objectives. The work set out to obtain materials based on calcium titanate via cold sintering process (CSP) using magnesium sulfate hydrate as an activating additive and study the phase composition, microstructure, integral structural characteristics, and dielectric properties of the obtained materials depending on the activating additive fraction and the CSP temperature. Methods. CaTiO 3 -based materials with additions of MgSO 4 ·6H 2 O (5–15 mol %) having an open porosity of at least 10% were obtained via CSP using uniaxial compression at a pressure of 220 MPa, temperatures from 300 to 400°C, and isothermal holding for 1 h. Results. A formation mechanism of the material under the specified conditions is proposed, including stages involving a predominance of dissolution–precipitation and solid-phase diffusion mechanisms. With the addition of 5–10 mol % of MgSO 4 ·6H 2 O, the dielectric loss tangent tanδ is ~0.01, while the relative permittivity ε r is 38–52 at frequencies from 500 kHz to 2 MHz. Increasing the CSP time to 2 h at 400°C leads to an increase in ε r to 50. Subsequent calcination in air at 900°C for 3 h leads to an increase in ε r to 62 and a decrease in tanδ to 0.004. The decrease in the ε r value of all the obtained materials as compared to pure CaTiO 3 (ε r = 150–170) is due to high open porosity values (at least 10%). Conclusions. A calcium titanate–based material via CSP can be produced using magnesium sulfate hydrate as an activating additive. CSP gives a porous material with high frequency stability, ε r = 38–62, and tanδ ~ 10 −2 –10 −3 . Due to their high open porosity, the resulting materials are promising for use as frameworks for composite capacitor materials.