Cerium oxide (CeO2) nanoparticles (NPs) was synthesized by the hydrothermal method. In this method cerium (IV) sulfate tetrahydrate as precursor was taken as solvent and sodium hydroxide as a precipitating agent. In this case, the CeO2 NPs were synthesized at various annealing conditions and characterized by different instrument techniques, including X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), High resolution transmission electron microscopy (HR-TEM), Energy dispersive X-ray analysis (EDAX) and Raman spectroscopy were employed to examine the crystal structure, functional groups, morphology and elemental composition of the final product. The dried and different calcination of the CeO2 NPs were investigated by supercapacitor and dielectric performance.
This study reports the synthesis of high dielectric constant zirconia oxide (ZrO2) nanorods (NRs) via a co-precipitation method followed by calcination at 700 °C for 2 h. X-ray diffraction (XRD) confirms a mixed-phase composition of orthorhombic and monoclinic structures, while transmission electron microscopy (TEM) reveals distinct nanorods. Energy dispersive X-ray analysis (EDAX) verifies the elemental composition. Photoluminescence (PL) spectroscopy indicates band gap energy of 1.9 eV, aligning better with orthorhombic zirconia. UV–vis analysis suggests oxygen vacancy defects potentially influencing the optical properties due to the nanorod morphology. Importantly, dielectric studies show a high dielectric constant of 29 at 1 MHz, which is approximately four times higher than commercially available ZrO2.
28 November 2023 in ECS Journal of Solid State Science and Technology
The special mixture morphology of the spherical and rod like the ZnO catalyst was successfully synthesized by a simple approach hydrothermal method. As the synthesized catalyst carried out by different conditions such as the ZnO dried, 250 °C and 500 °C calcination. Here, to investigated the calcination temperacture effect on crystal structure, phase, morphology and photocatalytic dye degraration with various dyes an including methylene blue (MB), methyl orange (MO), congo red (CR), and rhodamine b (RhB) under the direct Sunlight, was examined as manufactured ZnO catalysts. According to the results, all temperature conditions the ZnO have same crystal structure, phase, morphology and different performnce of the photocatalytic degradation with various dyes. Among these, the dried ZnO catalyst shown outstanding decolorization of the MB, MO, CR, and RhB dyes within 45 min followed by order percentages is about 100%, 93.89%, 98.18% and 96.98% respectively.