30 September 2024 in Progress on Chemistry and application of Chitin and its Derivatives
Bombyx mori chitosan nanoparticles (ChS NPs) were obtained and the kinetic aspects of their size distribution depending on the degree of nonequilibrium of the synthesis by ionotropic gelation using sodium tripolyphosphate (TPP) were studied. The size of ChS NPs was greatly influenced by the ChS concentration, which varied from 0.5 to 10 mg/ml. The size of the NPs increased from 100 to 300 nm when the ChS concentration increased from 0.5 to 10 mg/ml and while maintaining all other parameters of the reaction. An increase in the ChS to-TPP ratio corresponded to a lower cross-linking density and thus ensured slower kinetics for NP formation alongside the formation of large chitosan/TPP aggregates. There was an almost threefold increase in the particle size when the pH of the medium increased from 3.8 to 4.7; thus, the size of ChS NPs depends on the pH of the solution. There was a slight agglomeration of NPs from 363 to 642 nm with an increase in the NP synthesis time from 4 to 24 h. According to calculations, the maximum interaction energy is 50.4 and 69.4 kcal/mol for deprotonated TPP (P3O105-); after adiabatic transfer of the proton, the value decreases to 32.9–33.5 kcal/mol. The maximum interaction energy is –12.8 kcal/mol for the initially protonated TPP (H4P3O10-).
9 December 2025 in Eurasian Journal of Chemistry
The development of bioactive coatings combining biopolymers and calcium phosphate ceramics offers an effective strategy to improve osseointegration and functional performance of titanium-based implants. In this study, highly purified Bombyx mori chitosan (CS-BM) and β-tricalcium phosphate (β-TCP) were used to fabricate hybrid coatings on titanium substrates via electrochemical deposition under optimized conditions (52 °C, pH 6.6–7.0, 2.0–4.0 mA·cm–2). SEM and AFM analyses revealed uniform, strongly adherent two-layer structures with microtopography (1–10 μm roughness) favorable for bone ingrowth, while elemental analysis confirmed complete Ca- and P-rich coverage. Density functional theory (DFT) modeling confirmed the cooperative role of Ca2+ and PO43– in bridging CS-BM to TiO2, contributing to coating stability. In vivo studies demonstrated that CS-BM/TCP-coated implants accelerated early contact osteogenesis, dense trabecular bone formation, and stable bone–implant integration compared to uncoated controls. In an experimental osteoporosis model, intramuscular administration of CS-BM with active calcium or calcium–vitamin D3 significantly enhanced fibroblast-to-osteoblast differentiation, stimulated osteoid synthesis, and led to complete restoration of bone microarchitecture within 21 days. These findings highlight CS-BM/TCP coatings as a sustainable, locally sourced, and highly effective platform for orthopedic and dental implant applications, with additional therapeutic potential in osteoporosis management.