Nanofibers were prepared from polycaprolactone, polylactide and polyvinyl alcohol using NanospiderTM technology. Polyethylene glycols with molecular weights of 2 000, 6 000, 10 000 and 20 000 g/mol, which can be used to moderate the release profile of incorporated pharmacologically active compounds, served as model molecules. They were terminated by aromatic isocyanate and incorporated into the nanofibers. The release of these molecules into an aqueous environment was investigated. The influences of the molecular length and chemical composition of the nanofibers on the release rate and the amount of released polyethylene glycols were evaluated. Longer molecules released faster, as evidenced by a significantly higher amount of released molecules after 72 hours. However, the influence of the chemical composition of nanofibers was even more distinct – the highest amount of polyethylene glycol molecules released from polyvinyl alcohol nanofibers, the lowest amount from polylactide nanofibers.
The reaction of biphenylene with various nitriles in the presence of catalytic amount of [Rh(cod)2BF4]/dppe under microwave irradiation afforded 9-substituted phenanthridines. The reaction with alkyl and aromatic nitriles provided the corresponding 9-substituted phenanthridines in 26–79% isolated yields. The reaction was also carried out with cyanopyridines and it provided heterocyclic compounds with the bipyridine and terpyridine scaffold. The synthesized bipyridine and terpyridine were complexed with [Rh(cod)Cl]2. The former provided a Rh(III) complex in which the cyclooctadiene moiety was oxidized to the tetrahydrofuran ring, whereas the latter gave a structurally fluxional complex (in solution) with only one pyridine ring coordinated to the rhodium atom.