Maxillofacial prostheses are used in rehabilitation of patients with facial defects. Typically, these prostheses are fabricated with medical grade silicone and are tinted corresponding to the patients’ natural skin color. However, exposure to environment and disinfectants can result in color changes. This study aimed to evaluate the effects of four different disinfection methods on the color stability of precolored and hand-colored maxillofacial silicones. Forty specimens each of precolored and hand-colored silicone were prepared. The specimens were randomly divided into eight groups (n = 10) and cleansed with four different disinfection methods. Disinfection was carried out six times/day for 60 days, simulating once-a-day disinfection for a year. Color evaluation was carried out at day 0 and day 60 using a UV-vis spectrophotometer. Color alterations were calculated by the CIE system. Data were analyzed by two-way ANOVA with post hoc Tukey HSD and t-tests (α = 0.05). Disinfectants can affect the color stability of maxillofacial silicone. In our study, chlorhexidine solution and liquid soap resulted in the highest color change. Precolored silicone showed higher color stability than its hand-colored counterpart.
Long-term use of a denture base can be a reservoir of microbes due to porosities and mechanical wear of denture surfaces. Vanillin has an antimicrobial effect. However, its influence on physical properties after incorporated in PMMA has not yet been evaluated. The purpose of this study was to investigate physical properties of PMMA by incorporating vanillin in different concentrations. Material and method. There were three groups of PMMA with ten specimens per group. Flexural strength and flexural modulus were tested by using a 3-point bending machine, and surface hardness was determined by Vickers hardness test. One-way ANOVA and Kruskal Wallis tests were used to analyze all data at 0.05 significance level. Result. The 0.1% vanillin group yielded a significant difference in Vickers hardness number (17.15 HV) as compared to 0.5% vanillin group (16.30 HV) and without vanillin (15.30 HV). In contrast, the flexural strength and modulus showed no significant difference among test groups upon incorporation of vanillin. Conclusion. The vanillin incorporated PMMA group demonstrated higher surface hardness, compared to the group without vanillin. In addition, there were no significant differences in flexural strength and flexural modulus among the three groups. This study also found no adverse effect in physical properties of the vanillin incorporated PMMA.