This study evaluated the effect of an experimental paste containing hydroxyapatite in nanoparticles (nano-HA)/fluoride on dental de-remineralisation in situ. Thirteen subjects took part in this crossover/randomised/double-blind study performed in 4 phases (14 days each). Four sound and 4 pre-demineralised specimens were worn intraorally at each phase corresponding to the following treatments: Nanop Plus (10% HA, 0.2% NaF, nano-HA/fluoride), MI Paste Plus (casein phosphopeptide-amorphous calcium phosphate, 0.2% NaF), F (0.2% NaF) and placebo. Two-hundred and forty enamel and 240 dentine specimens were selected by using surface microhardness; half of them were subjected to pre-demineralisation and the other half remained sound. Sound specimens were further exposed to severe cariogenic challenge (20% sucrose in biofilm) in situ, while pre-demineralised specimens were not. All specimens were exposed to fluoride dentifrice slurry 2 × 1 min/day. Thereafter, the treatments were done for 4 min. The de-remineralisation was quantified by transversal microradiography. The data were statistically analysed by repeated-measures ANOVA/Tukey's tests (p < 0.05). Generally, no huge differences were found among the treatments. However, Nanop Plus was the only treatment able to significantly reduce dentine demineralisation (ΔZ, integrated mineral loss) and to improve enamel remineralisation (ΔΔZ, integrated mineral uptake) compared to placebo. No treatments were able to reduce enamel demineralisation, while for dentine remineralisation all treatments were similarly effective in improving ΔΔZ compared to placebo. Nanop Plus seems to have a positive influence on dental de-remineralisation, which should be further confirmed.
This in vitro study aimed to evaluate the action of TiF4 on sound and carious bovine and human enamel. Sound (S) and pre-demineralised (DE) bovine and human (primary and permanent) enamel samples were treated with TiF4 (pH 1.0) or NaF varnishes (pH 5.0), containing 0.95, 1.95, or 2.45% F for 12 h. The enamel surfaces were analysed using SEM-EDX (scanning electron microscopy/energy-dispersive X-ray spectroscopy) (n = 10, 5 S and 5 DE) and KOH-soluble fluoride was quantified (n = 20, 10 S and 10 DE). Hydroxyapatite powder produced by precipitation method was treated with the corresponding fluoride solutions for 1 min (n = 2). The formed compounds were detected using X-ray diffraction (XRD). All TiF4 varnishes produced a coating layer rich in Ti and F on all types of enamel surface, with micro-cracks in its extension. TiF4 (1.95 and 2.45% F) provided higher fluoride deposition than NaF, especially for bovine enamel (p < 0.0001). It also induced a higher fluoride deposition on DE samples compared to S samples (p < 0.0001), except for primary enamel. The Ti content was higher for bovine and human primary enamel than human permanent enamel, with some differences between S and DE. The XRD analysis showed that TiF4 induced the formation of new compounds such as CaF2, TiO2, and Ti(HPO4)2·H2O. In conclusion, TiF4 (>0.95% F) interacts better, when compared to NaF, with bovine and human primary enamel than with human permanent enamel. TiF4 provoked higher F deposition compared to NaF. Carious enamel showed higher F uptake than sound enamel by TiF4 application, while Ti uptake was dependent on the enamel condition and origin.
This in vitro study evaluated the preventive potential of experimental pastes containing 10% and 20% hydroxyapatite nanoparticles (Nano-HAP), with or without fluoride, on dental demineralization. Bovine enamel (n=15) and root dentin (n=15) specimens were divided into 9 groups according to their surface hardness: control (without treatment), 20 Nanop paste (20% HAP), 20 Nanop paste plus (20% HAP + 0.2% NaF), 10 Nanop paste (10% HAP), 10 Nanop paste plus (10% HAP + 0.2% NaF), placebo paste (without fluoride and HAP), fluoride paste (0.2% NaF), MI paste (CPP-ACP, casein phosphopeptide-amorphous calcium phosphate), and MI paste plus (CPP-ACP + 0.2% NaF). Both MI pastes were included as commercial control products containing calcium phosphate. The specimens were treated with the pastes twice a day (1 min), before and after demineralization. The specimens were subjected to a pH-cycling model (demineralization–6-8 h/ remineralization-16-18 h a day) for 7 days. The dental subsurface demineralization was analyzed using cross-sectional hardness (kgf/mm 2 , depth 10-220 µm). Data were tested using repeated-measures two-way ANOVA and Bonferroni's test (p<0.05). The only treatment able to reduce the loss of enamel and dentin subsurface hardness was fluoride paste (0.2% NaF), which differed significantly from the control at 30- and 50-µm depth (p<0.0001). The other treatments were not different from each other or compared with the control. The experimental Nanop pastes, regardless of the addition of fluoride, were unable to reduce dental demineralization in vitro.
22 February 2018 in Journal of Applied Oral Science
Titanium tetrafluoride (TiF4) is known for interacting with enamel reducing demineralization. However, no information is available about its potential antimicrobial effect.